Final Magnetic Moment8.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.059 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.091 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMoO2 |
Band Gap1.093 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/m [87] |
Hall-I 4 |
Point Group4/m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 1> | 246.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 173.4 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 104.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 242.7 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 312.1 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 147.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 242.7 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 242.7 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 312.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 69.3 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 173.4 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 138.7 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 294.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 173.4 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 277.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 112.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 343.3 |
BN (mp-984) | <0 0 1> | <1 0 0> | 277.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 118.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 277.4 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 208.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 34.7 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 118.1 |
MoS2 (mp-1434) | <0 0 1> | <1 1 0> | 343.3 |
Al (mp-134) | <1 0 0> | <1 0 0> | 173.4 |
Al (mp-134) | <1 1 0> | <1 1 0> | 294.2 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 343.3 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 245.2 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 208.0 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 294.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 173.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 104.0 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 312.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 277.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 312.1 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 208.0 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 346.7 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 225.7 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 343.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 173.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 294.2 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 294.2 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 98.1 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 245.2 |
LiTaO3 (mp-3666) | <1 0 1> | <1 0 0> | 312.1 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 196.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 225.7 |
TiO2 (mp-2657) | <0 0 1> | <1 1 0> | 196.1 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 312.1 |
TiO2 (mp-2657) | <1 1 0> | <1 1 0> | 98.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn3Cr3(SbO8)2 (mp-780598) | 0.4281 | 0.064 | 4 |
Ti3Fe3(SbO8)2 (mp-764329) | 0.3804 | 0.122 | 4 |
Ti3Mn3(SbO8)2 (mp-763292) | 0.4219 | 0.084 | 4 |
Mn3Cr3(TeO8)2 (mp-772458) | 0.3703 | 0.065 | 4 |
Ti3Cu3(TeO8)2 (mp-760579) | 0.4271 | 0.092 | 4 |
SnO2 (mvc-15363) | 0.3826 | 0.069 | 2 |
WO2 (mvc-2118) | 0.1599 | 0.111 | 2 |
CoO2 (mvc-14149) | 0.3667 | 0.000 | 2 |
CrO2 (mvc-12040) | 0.2837 | 0.067 | 2 |
VO2 (mp-25145) | 0.2252 | 0.046 | 2 |
Mn3(O2F)2 (mp-764666) | 0.2952 | 0.064 | 3 |
MnOF (mp-849587) | 0.3077 | 0.042 | 3 |
MnOF (mp-850984) | 0.3104 | 0.045 | 3 |
Mn3(O2F)2 (mp-764156) | 0.3229 | 0.062 | 3 |
Mn3(O2F)2 (mp-776690) | 0.3363 | 0.061 | 3 |
Li4ZrNb(TeO6)2 (mp-756177) | 0.7442 | 0.058 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-points64 |
U ValuesMo: 4.38 eV |
PseudopotentialsVASP PAW: Mo_pv O |
Final Energy/Atom-7.3254 eV |
Corrected Energy-107.6466 eV
-107.6466 eV = -87.9043 eV (uncorrected energy) - 14.1240 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)