Final Magnetic Moment0.369 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.234 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.461 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.58 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNi3O4 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [160] |
HallR 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 369.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 158.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 168.8 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 137.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 113.7 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 238.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 85.2 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 140.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 158.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 56.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 198.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 168.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 113.7 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 84.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 28.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 341.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 85.2 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 168.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 28.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 198.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 85.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 113.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 312.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 198.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 198.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 113.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 312.6 |
Al (mp-134) | <1 1 0> | <0 0 1> | 113.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 28.4 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 341.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 255.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 198.9 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 198.9 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 238.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 227.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 137.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 312.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 28.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 198.9 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 341.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 113.7 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 238.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 255.7 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 198.9 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 158.9 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 79.5 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 79.5 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 255.7 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 369.4 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 317.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
FeCo3O8 (mp-771554) | 0.1827 | 0.119 | 3 |
Li6Mn17O40 (mp-763817) | 0.3536 | 0.077 | 3 |
Mn6Zn3O16 (mp-774014) | 0.3863 | 0.355 | 3 |
Li2Mn5O12 (mp-763571) | 0.3562 | 0.310 | 3 |
LiMo3O8 (mp-25584) | 0.3051 | 0.213 | 3 |
CoO2 (mvc-12170) | 0.2711 | 0.213 | 2 |
CrO2 (mvc-14589) | 0.2578 | 0.191 | 2 |
CoO2 (mp-770908) | 0.1727 | 0.276 | 2 |
FeO2 (mvc-12125) | 0.2497 | 0.828 | 2 |
MnO2 (mvc-11093) | 0.1778 | 0.414 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Ni_pv O |
Final Energy/Atom-4.2699 eV |
Corrected Energy-65.5133 eV
-65.5133 eV = -51.2390 eV (uncorrected energy) - 8.6560 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)