Final Magnetic Moment8.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.150 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.473 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBa3Cr2O8 + BaCr2O4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmm2 [25] |
HallP 2 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 275.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 159.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 159.5 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 196.9 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 29.0 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 69.8 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 246.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 188.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 275.5 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 206.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 203.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 261.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 130.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 217.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 188.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 319.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 159.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 87.0 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 209.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 246.5 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 246.2 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 344.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 188.5 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 139.7 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 295.4 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 206.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 279.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 130.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 275.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 209.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 209.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 217.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 72.5 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 206.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 130.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 130.5 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 206.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 246.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 290.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 217.5 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 139.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 130.5 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 256.6 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 206.5 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 275.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 261.0 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 290.0 |
Te2W (mp-22693) | <1 0 1> | <1 1 0> | 209.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 261.0 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 344.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Ba_sv Cr_pv O |
Final Energy/Atom-6.8566 eV |
Corrected Energy-93.2346 eV
-93.2346 eV = -82.2796 eV (uncorrected energy) - 6.0390 eV (MP Advanced Correction) - 4.9160 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)