Final Magnetic Moment6.037 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.036 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.129 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa3Cr2(SiO4)3 + Cr2O3 + SiO2 |
Band Gap1.558 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP421c [114] |
HallP 4 2n |
Point Group42m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 0 0> | 229.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 329.1 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 253.9 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 161.9 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 329.1 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 161.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 274.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 274.2 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 274.2 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 161.9 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 109.7 |
C (mp-66) | <1 1 0> | <1 1 0> | 161.9 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 164.5 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 274.2 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 274.2 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 109.7 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 274.2 |
Si (mp-149) | <1 0 0> | <0 0 1> | 274.2 |
Au (mp-81) | <1 1 1> | <0 0 1> | 274.2 |
C (mp-48) | <1 0 0> | <1 0 0> | 114.5 |
WSe2 (mp-1821) | <1 0 0> | <1 0 1> | 253.9 |
WSe2 (mp-1821) | <1 1 0> | <1 0 1> | 253.9 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 54.8 |
ZrO2 (mp-2858) | <1 0 0> | <1 1 1> | 171.0 |
ZrO2 (mp-2858) | <1 0 1> | <1 1 1> | 171.0 |
ZrO2 (mp-2858) | <1 1 -1> | <1 0 0> | 229.0 |
ZrO2 (mp-2858) | <1 1 0> | <0 0 1> | 274.2 |
ZrO2 (mp-2858) | <1 1 1> | <1 0 1> | 253.9 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <0 0 1> | 109.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 274.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 274.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 164.5 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 161.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 274.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 274.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 274.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 219.4 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 114.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 54.8 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 229.0 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 219.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 219.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 219.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 274.2 |
BN (mp-984) | <1 0 0> | <1 0 0> | 114.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 274.2 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 329.1 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 219.4 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 164.5 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 229.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Ca_sv Cr_pv Si O |
Final Energy/Atom-7.7328 eV |
Corrected Energy-515.5781 eV
-515.5781 eV = -479.4345 eV (uncorrected energy) - 28.0916 eV (MP Anion Correction) - 8.0520 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)