Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.023 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.181 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaWO4 + CoO2 |
Band Gap0.498 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 48.8 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 69.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 146.5 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 119.3 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 1> | 244.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 85.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 170.1 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 198.8 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 79.5 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 195.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 120.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 85.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 255.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 255.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 368.6 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 159.1 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 318.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 85.1 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 278.3 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 119.3 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 321.2 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 139.0 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 159.1 |
SiO2 (mp-6930) | <0 0 1> | <1 0 -1> | 281.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 80.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 255.2 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 159.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 255.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 141.8 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 244.2 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 119.3 |
KCl (mp-23193) | <1 1 1> | <0 1 1> | 146.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 119.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 85.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 159.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 255.2 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 139.0 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 318.1 |
ZnSe (mp-1190) | <1 1 1> | <0 1 1> | 341.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 141.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 196.7 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 159.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 240.9 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 278.3 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 198.8 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 255.2 |
TePb (mp-19717) | <1 0 0> | <1 1 -1> | 226.0 |
TePb (mp-19717) | <1 1 1> | <0 1 1> | 146.5 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 200.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 226.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
PrMn2O6 (mvc-14396) | 0.2921 | 0.200 | 3 |
Pr(MoO3)2 (mvc-9652) | 0.2713 | 0.121 | 3 |
Pr(WO3)2 (mvc-9655) | 0.2970 | 0.181 | 3 |
Ca(WO3)2 (mvc-2131) | 0.1840 | 0.095 | 3 |
Ca(MoO3)2 (mvc-13363) | 0.2150 | 0.165 | 3 |
CaNiWO6 (mvc-12760) | 0.1798 | 0.250 | 4 |
CaMnWO6 (mvc-11373) | 0.1195 | 0.106 | 4 |
CaFeMoO6 (mvc-11007) | 0.2631 | 0.444 | 4 |
LaFeTeO6 (mvc-8907) | 0.2655 | 0.167 | 4 |
LaTaFeO6 (mvc-9007) | 0.2559 | 0.162 | 4 |
Bi2O5 (mvc-4554) | 0.6612 | 0.224 | 2 |
SbO2 (mp-560098) | 0.6767 | 0.001 | 2 |
SbO2 (mp-1819) | 0.7090 | 0.002 | 2 |
Bi3O7 (mvc-9064) | 0.6756 | 0.141 | 2 |
IrO3 (mp-1097041) | 0.6957 | 0.000 | 2 |
CaLa2Ti2Cr2O12 (mvc-13117) | 0.5579 | 0.098 | 5 |
CaNd2Ti2Mn2O12 (mvc-11950) | 0.5151 | 0.071 | 5 |
CaLa2Mn2(FeO6)2 (mvc-10933) | 0.5729 | 0.163 | 5 |
CaLa2Ti2Mn2O12 (mvc-14929) | 0.5677 | 0.132 | 5 |
BaNdNiSbO6 (mp-41829) | 0.6018 | 0.118 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eVW: 6.2 eV |
PseudopotentialsVASP PAW: Ca_sv Co W_pv O |
Final Energy/Atom-6.6141 eV |
Corrected Energy-139.9312 eV
-139.9312 eV = -119.0537 eV (uncorrected energy) - 12.4500 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)