Final Magnetic Moment16.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.035 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.111 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.16 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg2V2O7 + V4Fe2O13 + Fe2O3 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 330.8 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 327.4 |
CeO2 (mp-20194) | <1 1 0> | <1 -1 1> | 205.4 |
CeO2 (mp-20194) | <1 1 1> | <0 1 -1> | 202.5 |
BaF2 (mp-1029) | <1 1 0> | <0 1 -1> | 270.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 240.6 |
AlN (mp-661) | <1 0 0> | <0 1 -1> | 270.0 |
AlN (mp-661) | <1 0 1> | <1 -1 -1> | 197.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 275.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 327.4 |
InAs (mp-20305) | <1 1 0> | <0 1 -1> | 270.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 275.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 330.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 330.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 196.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 275.7 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 318.0 |
GaN (mp-804) | <1 0 1> | <1 -1 0> | 253.2 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 318.0 |
CdS (mp-672) | <1 0 0> | <0 1 -1> | 202.5 |
CdS (mp-672) | <1 1 0> | <0 1 -1> | 202.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 261.9 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 261.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 159.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 330.8 |
BN (mp-984) | <1 0 1> | <1 1 0> | 119.6 |
BN (mp-984) | <1 1 1> | <1 0 -1> | 238.5 |
LiNbO3 (mp-3731) | <1 0 1> | <1 1 0> | 239.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 275.7 |
MoS2 (mp-1434) | <1 0 0> | <1 -1 1> | 205.4 |
Al (mp-134) | <1 1 1> | <0 1 0> | 196.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 327.4 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 275.7 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 239.3 |
SiC (mp-7631) | <1 0 0> | <1 0 -1> | 318.0 |
SiC (mp-7631) | <1 0 1> | <1 0 -1> | 318.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 327.4 |
LiTaO3 (mp-3666) | <1 0 1> | <1 1 0> | 239.3 |
MgO (mp-1265) | <1 0 0> | <1 -1 0> | 253.2 |
MgO (mp-1265) | <1 1 0> | <1 -1 0> | 253.2 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 240.6 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 261.9 |
C (mp-66) | <1 1 0> | <0 1 -1> | 270.0 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 330.8 |
PbS (mp-21276) | <1 1 0> | <1 -1 0> | 253.2 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 275.7 |
GaP (mp-2490) | <1 1 0> | <1 -1 -1> | 296.7 |
GaP (mp-2490) | <1 1 1> | <0 1 -1> | 202.5 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 275.7 |
InP (mp-20351) | <1 1 0> | <1 -1 0> | 253.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr3(P2O7)2 (mp-569271) | 0.4571 | 0.001 | 3 |
Cr3(P2O7)2 (mp-774562) | 0.4563 | 0.001 | 3 |
Ni(PO3)2 (mp-19135) | 0.4599 | 0.000 | 3 |
Cr4P7O24 (mp-585323) | 0.4544 | 0.020 | 3 |
Cr2P3O11 (mp-31719) | 0.4020 | 0.016 | 3 |
V6Zn(FeO6)4 (mvc-12916) | 0.0899 | 0.116 | 4 |
LiP2WO8 (mp-765954) | 0.4064 | 0.065 | 4 |
LiV(OF)2 (mp-765509) | 0.4398 | 0.075 | 4 |
Fe2Ag(MoO4)3 (mp-565482) | 0.4081 | 0.030 | 4 |
LiV(PO4)2 (mp-32471) | 0.4431 | 0.064 | 4 |
FeO2 (mvc-11999) | 0.5881 | 0.372 | 2 |
CrO2 (mvc-11581) | 0.5998 | 0.166 | 2 |
VO2 (mp-777469) | 0.6384 | 0.038 | 2 |
VO2 (mvc-6918) | 0.5962 | 0.094 | 2 |
MoO2 (mvc-6944) | 0.5904 | 0.281 | 2 |
Li2MnV(PO4)3 (mp-771372) | 0.5384 | 0.039 | 5 |
Li2MnV(PO4)3 (mp-770134) | 0.5125 | 0.024 | 5 |
LiCrPO4F (mp-770575) | 0.4707 | 0.054 | 5 |
LiMnV(PO4)3 (mp-770143) | 0.4727 | 0.036 | 5 |
LiMnV(PO4)3 (mp-770057) | 0.5290 | 0.041 | 5 |
LiVCrP2(O4F)2 (mp-767223) | 0.6925 | 0.009 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.4969 | 0.255 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.6622 | 0.011 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.6125 | 0.330 | 6 |
Mn4Si4SnB2(HO9)2 (mp-743890) | 0.6733 | 0.000 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6829 | 0.002 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Mg_pv V_pv Fe_pv O |
Final Energy/Atom-6.9169 eV |
Corrected Energy-279.9705 eV
-279.9705 eV = -242.0915 eV (uncorrected energy) - 21.0240 eV (MP Advanced Correction) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)