Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.790 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.182 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.47 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMgFeSiO4 + SiO2 |
Band Gap3.592 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbca [61] |
Hall-P 2ac 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 144.0 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 294.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 336.1 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 109.4 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 196.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 240.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 167.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 336.1 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 218.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 336.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 144.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 288.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 240.1 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 174.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 144.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 218.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 288.1 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 336.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 288.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 167.8 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 196.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 336.1 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 240.1 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 144.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 288.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 336.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 336.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 336.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 48.0 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 1> | 218.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 336.1 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 240.1 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 336.1 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 336.1 |
C (mp-66) | <1 0 0> | <0 0 1> | 192.0 |
C (mp-66) | <1 1 1> | <0 0 1> | 288.1 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 288.1 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 167.8 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 336.1 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 336.1 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 240.1 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 336.1 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 336.1 |
ZrO2 (mp-2858) | <0 0 1> | <0 1 1> | 109.4 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 336.1 |
ZrO2 (mp-2858) | <0 1 1> | <0 1 0> | 196.6 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 144.0 |
ZrO2 (mp-2858) | <1 0 1> | <0 1 1> | 218.8 |
ZrO2 (mp-2858) | <1 1 0> | <0 0 1> | 240.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 288.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnFe(SiO3)2 (mvc-6883) | 0.1496 | 0.051 | 4 |
MgCr(SiO3)2 (mvc-6880) | 0.1206 | 0.770 | 4 |
ZnCr(SiO3)2 (mvc-6877) | 0.1275 | 0.095 | 4 |
MgCo(SiO3)2 (mvc-6878) | 0.1019 | 0.015 | 4 |
MgFe(SiO3)2 (mvc-14507) | 0.0808 | 0.182 | 4 |
MoO2 (mvc-6944) | 0.7081 | 0.387 | 2 |
MgSiO3 (mp-5834) | 0.2481 | 0.026 | 3 |
MgSiO3 (mp-1020123) | 0.2394 | 0.039 | 3 |
MgSiO3 (mp-3470) | 0.3005 | 0.006 | 3 |
FeSiO3 (mp-630331) | 0.2976 | 0.038 | 3 |
CoSiO3 (mp-699575) | 0.2358 | 0.020 | 3 |
NaLi7Fe8(SiO3)16 (mp-775490) | 0.5379 | 0.011 | 5 |
Li4MnV(PO4)3 (mp-770137) | 0.5638 | 0.026 | 5 |
Li3MnV(P2O7)2 (mp-850951) | 0.5245 | 0.000 | 5 |
Li2MnV4NiO12 (mp-868654) | 0.5589 | 0.064 | 5 |
Li3VCr(P2O7)2 (mp-765133) | 0.5354 | 0.018 | 5 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.6905 | 0.041 | 6 |
Na2Gd2MgSi4(O6F)2 (mp-557538) | 0.7219 | 0.000 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.7381 | 0.028 | 6 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.6145 | 0.008 | 6 |
CaMg2TiAl2SiO10 (mp-534863) | 0.6773 | 0.026 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.7414 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Mg_pv Fe_pv Si O |
Final Energy/Atom-7.1553 eV |
Corrected Energy-627.9983 eV
-627.9983 eV = -572.4244 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 21.8640 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)