Final Magnetic Moment0.990 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.408 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.92 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 353.9 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 118.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 175.6 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 196.6 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 83.8 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 196.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 87.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 322.0 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 118.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 87.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 263.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 29.3 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 335.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 83.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 255.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 146.4 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 255.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 125.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 167.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 87.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 263.5 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 157.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 125.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 87.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 322.0 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 125.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 263.5 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 209.5 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 322.4 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 196.1 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 196.1 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 255.6 |
TePb (mp-19717) | <1 1 1> | <0 1 1> | 147.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 153.3 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 275.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 322.0 |
GaSe (mp-1943) | <1 0 1> | <1 0 1> | 204.4 |
BN (mp-984) | <1 0 0> | <1 1 0> | 57.5 |
BN (mp-984) | <1 1 1> | <1 1 0> | 229.8 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 146.4 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 255.6 |
MoS2 (mp-1434) | <1 0 0> | <0 1 1> | 196.1 |
Al (mp-134) | <1 1 0> | <0 0 1> | 87.8 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 1> | 245.1 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 51.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 125.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 125.7 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 322.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 117.1 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 125.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SmTiO3 (mp-22416) | 0.0942 | 0.060 | 3 |
TbNiO3 (mp-769876) | 0.0664 | 0.000 | 3 |
GdTiO3 (mp-510278) | 0.0984 | 0.027 | 3 |
TbCoO3 (mp-24881) | 0.0967 | 0.000 | 3 |
SmTiO3 (mp-561777) | 0.0958 | 0.060 | 3 |
Sm2MgIrO6 (mp-980108) | 0.1058 | 0.006 | 4 |
Tb2MnNiO6 (mp-645135) | 0.1107 | 0.000 | 4 |
Y2MnNiO6 (mp-19192) | 0.1241 | 0.000 | 4 |
LiSm2IrO6 (mp-11904) | 0.1451 | 0.000 | 4 |
LiNd2IrO6 (mp-11905) | 0.1555 | 0.000 | 4 |
Mn3O4 (mp-25696) | 0.7298 | 0.053 | 2 |
Al2O3 (mp-642363) | 0.6652 | 0.280 | 2 |
Cr3C2 (mp-570112) | 0.6710 | 0.030 | 2 |
Fe2O3 (mp-1078361) | 0.7337 | 0.704 | 2 |
Mn3O4 (mp-715570) | 0.7178 | 0.053 | 2 |
CaSmMnSnO6 (mp-698702) | 0.2849 | 0.176 | 5 |
LiLaNdSbO6 (mp-776091) | 0.2576 | 0.006 | 5 |
CaLaTaFeO6 (mvc-9005) | 0.2964 | 0.000 | 5 |
CaLaFeAgO6 (mvc-8977) | 0.2672 | 0.054 | 5 |
CaLaMnRuO6 (mp-690556) | 0.2700 | 0.080 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Y_sv Ni_pv O |
Final Energy/Atom-6.9719 eV |
Corrected Energy-157.8464 eV
Uncorrected energy = -139.4384 eV
Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV
Composition-based energy adjustment (-2.541 eV/atom x 4.0 atoms) = -10.1640 eV
Corrected energy = -157.8464 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)