Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.759 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.008 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.36 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa4P6O19 + Co3(PO4)2 + Ca2P2O7 |
Band Gap2.854 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 -1> | 130.4 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 -1> | 130.4 |
AlN (mp-661) | <0 0 1> | <1 -1 -1> | 160.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 171.4 |
AlN (mp-661) | <1 0 1> | <0 1 -1> | 142.0 |
AlN (mp-661) | <1 1 0> | <0 1 -1> | 189.3 |
AlN (mp-661) | <1 1 1> | <1 1 -1> | 260.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 120.8 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 289.4 |
CeO2 (mp-20194) | <1 1 1> | <1 1 -1> | 326.0 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 322.2 |
GaN (mp-804) | <0 0 1> | <1 1 -1> | 260.8 |
GaN (mp-804) | <1 0 0> | <1 -1 0> | 167.4 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 188.1 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 120.8 |
SiO2 (mp-6930) | <0 0 1> | <0 1 -1> | 283.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 214.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 217.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 282.0 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 294.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 201.4 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 201.4 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 201.4 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 256.0 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 161.1 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 161.1 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 322.2 |
TePb (mp-19717) | <1 0 0> | <1 1 -1> | 130.4 |
Te2Mo (mp-602) | <0 0 1> | <0 1 -1> | 142.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 -1 1> | 294.6 |
BN (mp-984) | <1 0 0> | <0 1 1> | 217.1 |
BN (mp-984) | <1 1 1> | <1 -1 0> | 279.1 |
LiNbO3 (mp-3731) | <1 1 0> | <1 1 1> | 256.0 |
MoS2 (mp-1434) | <0 0 1> | <1 -1 1> | 176.8 |
Al (mp-134) | <1 0 0> | <1 0 0> | 201.4 |
Al (mp-134) | <1 1 0> | <1 0 0> | 161.1 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 282.0 |
LiGaO2 (mp-5854) | <1 0 1> | <1 -1 0> | 279.1 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 201.4 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 1> | 217.1 |
TeO2 (mp-2125) | <0 0 1> | <0 1 1> | 289.4 |
TeO2 (mp-2125) | <0 1 0> | <1 -1 0> | 279.1 |
TeO2 (mp-2125) | <1 0 0> | <1 -1 0> | 279.1 |
TeO2 (mp-2125) | <1 0 1> | <1 1 -1> | 326.0 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 201.4 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 -1> | 326.0 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 0> | 305.1 |
LiTaO3 (mp-3666) | <1 1 0> | <1 1 1> | 256.0 |
LiTaO3 (mp-3666) | <1 1 1> | <1 1 1> | 256.0 |
MgO (mp-1265) | <1 0 0> | <0 1 -1> | 236.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe3(P2O7)2 (mvc-12221) | 0.5680 | 0.327 | 3 |
V3(P2O7)2 (mp-32416) | 0.5332 | 0.033 | 3 |
V3(P2O7)2 (mvc-15147) | 0.5800 | 0.033 | 3 |
Si2Sn2O7 (mp-769046) | 0.4175 | 0.086 | 3 |
Fe3(P2O7)2 (mp-540486) | 0.5718 | 0.327 | 3 |
CaFeP2O7 (mvc-5578) | 0.1394 | 0.000 | 4 |
CaTiP2O7 (mvc-5356) | 0.1471 | 0.215 | 4 |
CaCoP2O7 (mvc-15045) | 0.1400 | 0.008 | 4 |
CaNiP2O7 (mvc-12078) | 0.1507 | 0.000 | 4 |
CaNiP2O7 (mp-19057) | 0.1503 | 0.000 | 4 |
K2Mn2P2O7F2 (mp-566013) | 0.5260 | 0.000 | 5 |
Na2ZrNi(P2O7)2 (mp-18984) | 0.5478 | 0.058 | 5 |
Na2ZrCo(P2O7)2 (mp-19187) | 0.5364 | 0.030 | 5 |
SrMgV(PO4)2 (mvc-2997) | 0.5642 | 0.025 | 5 |
SrVZn(PO4)2 (mvc-2998) | 0.5511 | 0.033 | 5 |
Ca6Ti5AlSi6O29F (mp-693358) | 0.6862 | 0.008 | 6 |
Na2Gd2MgSi4(O6F)2 (mp-557538) | 0.4935 | 0.000 | 6 |
NaCa8SmTi10(SiO5)10 (mp-705853) | 0.7142 | 0.002 | 6 |
NaLiMn2Fe4(PO4)6 (mp-777193) | 0.6199 | 0.018 | 6 |
NaInBP2HO9 (mp-757312) | 0.6984 | 0.013 | 6 |
Na2Ca4ZrNbSi4O17F (mp-6903) | 0.7191 | 0.000 | 7 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6108 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Ca_sv Co P O |
Final Energy/Atom-7.1033 eV |
Corrected Energy-169.8534 eV
-169.8534 eV = -156.2733 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction) - 3.7480 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)