Final Magnetic Moment6.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.663 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.121 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToYCrO4 + YCrO3 + Cr2O3 |
Band Gap0.011 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 119.0 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 171.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 198.4 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 283.7 |
BaF2 (mp-1029) | <1 1 1> | <0 1 1> | 283.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 317.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 277.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 246.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 257.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 158.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 257.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 357.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 277.7 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 283.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 317.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 238.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 158.7 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 171.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 158.7 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 119.0 |
TePb (mp-19717) | <1 1 1> | <1 1 0> | 150.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 277.7 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 158.7 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 277.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 317.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 198.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 198.4 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 277.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 198.4 |
BN (mp-984) | <1 0 0> | <0 1 0> | 171.5 |
BN (mp-984) | <1 0 1> | <0 1 1> | 283.7 |
BN (mp-984) | <1 1 0> | <0 0 1> | 198.4 |
BN (mp-984) | <1 1 1> | <0 0 1> | 357.1 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 150.3 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 277.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 198.4 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 246.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 317.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 119.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 123.3 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 85.8 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 85.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 317.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 317.4 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 158.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 119.0 |
KCl (mp-23193) | <1 1 1> | <0 1 1> | 283.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 357.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 1> | 94.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 277.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Y2(NiO3)3 (mvc-12303) | 0.3049 | 0.262 | 3 |
Y2V3O9 (mvc-14376) | 0.1643 | 0.095 | 3 |
Nd9Ti10O30 (mp-532477) | 0.4818 | 0.023 | 3 |
Y2Mn3O9 (mvc-14400) | 0.2618 | 0.121 | 3 |
Y2Ti3O9 (mvc-12320) | 0.1807 | 0.045 | 3 |
Ca3Mn2(SbO6)2 (mvc-10908) | 0.3700 | 0.146 | 4 |
Ca3Co2(TeO6)2 (mvc-12889) | 0.3645 | 0.136 | 4 |
Ca3Fe2(ReO6)2 (mvc-12765) | 0.3575 | 0.026 | 4 |
Ca3Fe2(MoO6)2 (mvc-12764) | 0.3815 | 0.075 | 4 |
Ca3Fe2(SbO6)2 (mvc-14981) | 0.3355 | 0.121 | 4 |
CaNd2Ti2Mn2O12 (mvc-11950) | 0.5109 | 0.071 | 5 |
LaMgTiFeO6 (mvc-8879) | 0.5419 | 0.093 | 5 |
LaMgVCrO6 (mvc-9838) | 0.5397 | 0.744 | 5 |
LaVZnCrO6 (mvc-9860) | 0.5388 | 0.148 | 5 |
LaMgCrNiO6 (mvc-9871) | 0.5439 | 0.695 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Y_sv Cr_pv O |
Final Energy/Atom-7.9536 eV |
Corrected Energy-494.8396 eV
-494.8396 eV = -445.4011 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction) - 24.1560 eV (MP Advanced Correction)
|