Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.055 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.109 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.22 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa3VN3 + V2N + Ca |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 338.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 333.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 55.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 166.5 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 218.8 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 77.3 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 348.5 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 323.0 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 348.5 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 231.9 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 291.8 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 304.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 277.5 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 291.8 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 203.3 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 85.2 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 304.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 55.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 277.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 348.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 323.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 237.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 255.5 |
CdS (mp-672) | <0 0 1> | <1 1 -1> | 244.7 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 237.1 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 199.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 199.1 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 169.4 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 255.5 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 237.1 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 258.4 |
YVO4 (mp-19133) | <1 1 0> | <1 0 -1> | 199.1 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 154.6 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 135.5 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 291.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 291.8 |
Te2Mo (mp-602) | <1 1 1> | <1 1 0> | 291.8 |
Ag (mp-124) | <1 0 0> | <1 1 -1> | 244.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 222.0 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 203.3 |
GaSe (mp-1943) | <1 1 1> | <1 0 0> | 237.1 |
BN (mp-984) | <1 0 0> | <1 0 1> | 77.3 |
BN (mp-984) | <1 1 1> | <1 0 1> | 309.2 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 101.6 |
GaSe (mp-1943) | <1 1 0> | <1 0 0> | 237.1 |
BN (mp-984) | <0 0 1> | <1 1 0> | 218.8 |
BN (mp-984) | <1 0 1> | <1 0 0> | 169.4 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 -1> | 149.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 -1> | 244.7 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 1> | 231.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2CrN2 (mvc-15308) | 0.2232 | 0.076 | 3 |
Ca2MnN2 (mvc-14557) | 0.2961 | 0.048 | 3 |
Ca2WN2 (mvc-13792) | 0.2697 | 0.000 | 3 |
Ca2FeN2 (mp-28770) | 0.4503 | 0.076 | 3 |
Ca2TiN2 (mvc-15307) | 0.3146 | 0.122 | 3 |
Li2VO3F (mp-765755) | 0.7261 | 0.103 | 4 |
Li2Mn2OF6 (mp-765120) | 0.5995 | 0.073 | 4 |
TiZnBiO5 (mvc-7457) | 0.7074 | 0.077 | 4 |
CaSnBiO5 (mvc-9023) | 0.7197 | 0.099 | 4 |
Mg2BiWO6 (mvc-5927) | 0.7156 | 0.133 | 4 |
V4O7 (mp-715493) | 0.7048 | 0.274 | 2 |
Li4Ti4V4NiO18 (mp-769451) | 0.7360 | 0.082 | 5 |
Li4Ti4V4CoO18 (mp-769478) | 0.7268 | 0.092 | 5 |
Li4Ti4Mn(Fe2O9)2 (mp-769443) | 0.7359 | 0.087 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv V_pv N |
Final Energy/Atom-6.8519 eV |
Corrected Energy-68.5192 eV
-68.5192 eV = -68.5192 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)