Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.055 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.069 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.36 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSnO2 |
Band Gap1.783 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/m [87] |
Hall-I 4 |
Point Group4/m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 173.7 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 245.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 115.5 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 120.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 312.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 294.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 312.6 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 120.6 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 245.6 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 294.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 243.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 173.7 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 312.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 294.8 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 347.4 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 347.4 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 196.5 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 208.4 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 294.8 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 312.6 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 312.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 343.9 |
BN (mp-984) | <1 0 0> | <1 0 0> | 277.9 |
BN (mp-984) | <1 0 1> | <1 1 0> | 245.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 243.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 208.4 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 343.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 34.7 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 243.2 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 312.6 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 0> | 312.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 347.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 208.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 104.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 277.9 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 173.7 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 312.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 69.5 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 98.3 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 139.0 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 243.2 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 139.0 |
BN (mp-984) | <0 0 1> | <1 1 1> | 125.5 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 34.7 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 69.5 |
Al (mp-134) | <1 1 0> | <1 1 0> | 294.8 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 245.6 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 0> | 98.3 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 208.4 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 343.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe3(O2F)2 (mp-780093) | 0.2480 | 0.643 | 3 |
Ni3OF5 (mp-763929) | 0.2650 | 0.071 | 3 |
Mn3O5F (mp-777654) | 0.2478 | 0.062 | 3 |
Ni3OF5 (mp-763299) | 0.2696 | 0.066 | 3 |
Ni3OF5 (mp-763215) | 0.2715 | 0.070 | 3 |
LiV3(OF3)2 (mp-868491) | 0.2738 | 0.000 | 4 |
LiFe2OF5 (mp-779300) | 0.3104 | 0.244 | 4 |
Mn3Co3(SbO8)2 (mp-863857) | 0.3088 | 0.300 | 4 |
LiCo3(OF3)2 (mp-850982) | 0.2753 | 0.022 | 4 |
Ta2CrNO5 (mp-849504) | 0.3032 | 0.065 | 4 |
FeO2 (mvc-12905) | 0.1403 | 0.354 | 2 |
CrO2 (mvc-12040) | 0.0822 | 0.121 | 2 |
MnO2 (mvc-12022) | 0.1182 | 0.000 | 2 |
CoO2 (mvc-14149) | 0.0766 | 0.000 | 2 |
MnO2 (mp-19395) | 0.1202 | 0.000 | 2 |
Explore more synthesis descriptions for materials of composition SnO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sn_d O |
Final Energy/Atom-6.2160 eV |
Corrected Energy-80.2108 eV
-80.2108 eV = -74.5925 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)