Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.006 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.324 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZn2CrN3 + CrN + Zn |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 170.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 113.5 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 158.6 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 197.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 138.9 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 198.7 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 227.1 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 141.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 185.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 211.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 277.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 282.0 |
CeO2 (mp-20194) | <1 0 0> | <1 1 -1> | 331.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 356.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 356.9 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 318.9 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 113.5 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 318.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 356.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 255.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 231.5 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 170.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 324.1 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 119.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 231.5 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 265.8 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 169.2 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 212.6 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 301.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 324.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 237.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 263.1 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 283.9 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 283.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 317.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 317.2 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 227.1 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 158.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 356.9 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 318.9 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 263.1 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 119.0 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 198.3 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 197.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 198.7 |
GaSe (mp-1943) | <1 0 1> | <1 0 0> | 141.9 |
BN (mp-984) | <1 0 1> | <1 1 -1> | 198.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 85.2 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 198.7 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 227.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn2WN2 (mvc-13731) | 0.6007 | 0.503 | 3 |
BiSI (mp-23514) | 0.6233 | 0.003 | 3 |
AsSeI (mp-505373) | 0.6150 | 0.000 | 3 |
Ag2SeO3 (mp-16913) | 0.5480 | 0.000 | 3 |
CuGeI3 (mp-1096949) | 0.5886 | 0.255 | 3 |
RbEuAsS3 (mp-646129) | 0.6996 | 0.000 | 4 |
BiTeIO3 (mp-559332) | 0.6366 | 0.007 | 4 |
CoSb2Br2O3 (mp-561493) | 0.7435 | 0.000 | 4 |
LaCuTeS (mp-10288) | 0.7301 | 0.000 | 4 |
AgAsPbS3 (mp-22665) | 0.7458 | 0.000 | 4 |
Bi2O3 (mp-556549) | 0.7421 | 0.024 | 2 |
Sb2S3 (mp-2809) | 0.7203 | 0.000 | 2 |
BiSe2 (mp-1095302) | 0.6243 | 0.041 | 2 |
BiS2 (mp-971673) | 0.6751 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zn Cr_pv N |
Final Energy/Atom-5.6209 eV |
Corrected Energy-56.2093 eV
-56.2093 eV = -56.2093 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)