Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.125 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.132 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.35 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLa6WO12 + W + MgO + La2WO6 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-P 3* |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 345.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 259.1 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 252.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 230.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 316.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 201.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 168.1 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 136.7 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 201.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 201.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 115.1 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 236.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 345.4 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 115.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 86.4 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 139.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 201.5 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 259.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 201.5 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 78.9 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 78.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 157.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 230.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 168.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 201.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 168.1 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 136.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 143.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 115.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 28.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 316.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 201.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 236.8 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 345.4 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 84.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 115.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 28.8 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 201.5 |
C (mp-66) | <1 0 0> | <0 0 1> | 201.5 |
C (mp-66) | <1 1 0> | <0 0 1> | 143.9 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 157.9 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 230.3 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 57.6 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 115.1 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 236.8 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 315.8 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 259.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 201.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 86.4 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 168.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La2MgSnO6 (mvc-13582) | 0.0851 | 0.033 | 4 |
La2MgMoO6 (mvc-15456) | 0.0504 | 0.045 | 4 |
La2ZnWO6 (mvc-15420) | 0.1271 | 0.178 | 4 |
La2TiZnO6 (mvc-11053) | 0.1055 | 0.060 | 4 |
La2ZnMoO6 (mvc-11208) | 0.1118 | 0.088 | 4 |
SnO2 (mvc-15363) | 0.6438 | 0.069 | 2 |
MnO2 (mp-19326) | 0.6474 | 0.008 | 2 |
TiO2 (mp-766454) | 0.6298 | 0.059 | 2 |
SiO2 (mp-32667) | 0.6391 | 0.243 | 2 |
ZrO2 (mp-776386) | 0.6309 | 0.090 | 2 |
PrTiO3 (mp-753948) | 0.1439 | 0.022 | 3 |
LuAlO3 (mp-754435) | 0.0728 | 0.082 | 3 |
BaPrO3 (mp-6910) | 0.0784 | 0.114 | 3 |
BaNdO3 (mp-754307) | 0.1216 | 0.118 | 3 |
TbNiO3 (mp-770347) | 0.1323 | 0.043 | 3 |
SrLaMnRuO6 (mp-39239) | 0.3069 | 0.000 | 5 |
NaLa2Ti2MnO9 (mp-690559) | 0.4997 | 0.029 | 5 |
CaLa9Ti5Cr5O30 (mp-694926) | 0.4169 | 0.059 | 5 |
Ca2La8Ti5Cr5O30 (mp-743953) | 0.3534 | 0.040 | 5 |
SrLa7TiGa7O24 (mp-720505) | 0.4394 | 0.043 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-points38 |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: La Mg_pv W_pv O |
Final Energy/Atom-7.6703 eV |
Corrected Energy-85.2675 eV
-85.2675 eV = -76.7028 eV (uncorrected energy) - 4.3510 eV (MP Advanced Correction) - 4.2137 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)