Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.169 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.129 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.11 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg4Sb2O9 + Mg(SbO3)2 + Mg(CoO2)2 |
Band Gap0.431 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 148.0 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 84.0 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 81.2 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 40.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 196.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 284.3 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 84.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 81.2 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 140.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 157.1 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 121.8 |
KCl (mp-23193) | <1 1 1> | <0 1 1> | 144.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 162.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 252.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 157.1 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 324.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 284.3 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 49.3 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 140.0 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 345.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 280.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 243.6 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 121.8 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 0> | 246.6 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 168.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 196.4 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 193.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 117.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 162.4 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 224.0 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 246.6 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 341.2 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 364.0 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 224.0 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 252.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 117.9 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 324.8 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 280.0 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 284.2 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 252.0 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 246.6 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 140.0 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 157.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 121.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 84.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 157.1 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 227.5 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 121.8 |
TePb (mp-19717) | <1 1 1> | <0 1 1> | 144.7 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 157.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnZnO3 (mvc-3995) | 0.2699 | 0.098 | 3 |
MgSnO3 (mvc-15649) | 0.2525 | 0.073 | 3 |
ZnFeO3 (mvc-14155) | 0.2095 | 0.159 | 3 |
HfMnO3 (mp-776496) | 0.2715 | 0.032 | 3 |
LuTlO3 (mp-754597) | 0.2683 | 0.084 | 3 |
Mg2CrSbO6 (mvc-13423) | 0.1320 | 0.710 | 4 |
Zn2CrSbO6 (mvc-15620) | 0.1688 | 0.093 | 4 |
Mg2TiSbO6 (mvc-15346) | 0.1748 | 0.171 | 4 |
Mg2VSbO6 (mvc-14653) | 0.0721 | 0.123 | 4 |
Mg2FeSbO6 (mvc-13829) | 0.0645 | 0.269 | 4 |
V3O5 (mp-714914) | 0.6033 | 0.004 | 2 |
V3O5 (mp-542441) | 0.5801 | 0.029 | 2 |
Ti3O5 (mp-556754) | 0.5690 | 0.013 | 2 |
Ti4O7 (mp-12205) | 0.6089 | 0.005 | 2 |
Ti4O7 (mp-558097) | 0.6071 | 0.005 | 2 |
Li4CrTe(WO6)2 (mp-777147) | 0.5239 | 0.075 | 5 |
Mg3AlFe(SiO4)3 (mp-699146) | 0.5118 | 0.311 | 5 |
Li4CrBi(TeO6)2 (mp-775998) | 0.5319 | 0.076 | 5 |
LaMgCrSbO6 (mvc-9859) | 0.5245 | 0.842 | 5 |
LaMgCrSnO6 (mvc-9925) | 0.5284 | 0.773 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Mg_pv Co Sb O |
Final Energy/Atom-5.9723 eV |
Corrected Energy-131.6222 eV
-131.6222 eV = -119.4467 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 3.7480 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)