material

WO3

ID:

mvc-15643

DOI:

10.17188/1319514


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.171 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.003 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.90 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
WO3
Band Gap
1.496 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P212121 [19]
Hall
P 2ac 2ab
Point Group
222
Crystal System
orthorhombic
We have not yet calculated a detailed bandstructure for this material

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CeO2 (mp-20194) <1 1 1> <0 1 0> 0.004 206.2
Si (mp-149) <1 1 1> <0 1 0> 0.005 206.2
Te2Mo (mp-602) <1 0 0> <0 1 0> 0.012 164.9
InSb (mp-20012) <1 1 0> <1 0 0> 0.020 125.2
CaCO3 (mp-3953) <1 0 0> <1 1 1> 0.022 261.6
CdTe (mp-406) <1 1 0> <1 0 0> 0.025 125.2
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.037 260.3
MgO (mp-1265) <1 0 0> <0 0 1> 0.037 144.6
TiO2 (mp-390) <0 0 1> <0 0 1> 0.037 28.9
LaAlO3 (mp-2920) <1 1 1> <0 1 1> 0.038 251.8
KP(HO2)2 (mp-23959) <1 0 0> <0 0 1> 0.038 115.7
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.039 144.6
PbS (mp-21276) <1 0 0> <0 0 1> 0.047 144.6
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.047 144.6
KTaO3 (mp-3614) <1 1 0> <1 0 0> 0.048 250.4
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.049 144.6
NaCl (mp-22862) <1 0 0> <0 0 1> 0.051 260.3
C (mp-66) <1 0 0> <0 0 1> 0.057 115.7
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.057 260.3
LaAlO3 (mp-2920) <1 1 0> <1 0 0> 0.063 125.2
C (mp-48) <1 1 0> <0 1 0> 0.064 164.9
GaP (mp-2490) <1 1 1> <0 1 0> 0.064 206.2
Al (mp-134) <1 0 0> <0 0 1> 0.066 144.6
GaAs (mp-2534) <1 0 0> <0 0 1> 0.071 260.3
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.074 28.9
LaAlO3 (mp-2920) <0 0 1> <0 1 1> 0.074 50.4
CdTe (mp-406) <1 1 1> <0 1 1> 0.075 151.1
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.075 289.3
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.077 260.3
InSb (mp-20012) <1 1 1> <0 1 1> 0.077 151.1
Cu (mp-30) <1 0 0> <0 0 1> 0.078 115.7
AlN (mp-661) <0 0 1> <0 1 1> 0.079 50.4
WSe2 (mp-1821) <1 1 0> <1 1 1> 0.081 261.6
Al (mp-134) <1 1 0> <1 0 0> 0.083 250.4
C (mp-48) <0 0 1> <0 1 1> 0.090 100.7
CaF2 (mp-2741) <1 1 1> <0 1 0> 0.090 206.2
GaSe (mp-1943) <0 0 1> <0 0 1> 0.092 202.5
PbSe (mp-2201) <1 1 0> <0 1 0> 0.094 164.9
YAlO3 (mp-3792) <1 0 0> <0 1 1> 0.097 201.5
Cu (mp-30) <1 1 0> <0 1 0> 0.098 164.9
GaSb (mp-1156) <1 1 0> <0 1 0> 0.099 164.9
ZrO2 (mp-2858) <1 0 1> <0 0 1> 0.099 86.8
Ge (mp-32) <1 0 0> <0 0 1> 0.100 260.3
Te2Mo (mp-602) <0 0 1> <0 1 1> 0.103 151.1
Te2Mo (mp-602) <1 0 1> <0 1 0> 0.103 164.9
CdSe (mp-2691) <1 1 0> <0 1 0> 0.105 164.9
SiC (mp-11714) <1 1 0> <0 1 0> 0.109 164.9
BN (mp-984) <1 1 0> <0 1 0> 0.111 164.9
ZnO (mp-2133) <1 1 0> <0 1 0> 0.111 123.7
SiC (mp-8062) <1 1 1> <0 1 1> 0.114 100.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
142 37 -10 0 0 0
37 105 -11 0 0 0
-10 -11 80 0 0 0
0 0 0 64 0 0
0 0 0 0 103 0
0 0 0 0 0 52
Compliance Tensor Sij (10-12Pa-1)
7.8 -2.7 0.6 0 0 0
-2.7 10.6 1.1 0 0 0
0.6 1.1 12.8 0 0 0
0 0 0 15.6 0 0
0 0 0 0 9.7 0
0 0 0 0 0 19.4
Shear Modulus GV
64 GPa
Bulk Modulus KV
40 GPa
Shear Modulus GR
57 GPa
Bulk Modulus KR
34 GPa
Shear Modulus GVRH
61 GPa
Bulk Modulus KVRH
37 GPa
Elastic Anisotropy
0.80
Poisson's Ratio
-0.03

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 -0.04045 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 0.21765 0.00000
0.00000 0.00000 0.00000 0.00000 0.00000 -0.00170
Piezoelectric Modulus ‖eijmax
0.21765 C/m2
Crystallographic Direction vmax
0.00000
1.00000
-0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
6.05 0.00 0.00
0.00 7.00 0.00
0.00 0.00 6.86
Dielectric Tensor εij (total)
32.12 0.00 0.02
0.00 466.33 0.03
0.02 0.03 364.11
Polycrystalline dielectric constant εpoly
(electronic contribution)
6.63
Polycrystalline dielectric constant εpoly
(total)
287.52
Refractive Index n
2.58
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
V4(OF3)3 (mp-853156) 0.3552 0.006 3
NbO2F (mp-752467) 0.3588 0.000 3
V2OF5 (mp-778686) 0.3348 0.016 3
V4(OF3)3 (mp-775103) 0.3807 0.018 3
V2OF5 (mp-763048) 0.3423 0.018 3
FeAg3(CN)6 (mp-568663) 0.7014 0.307 4
Cs2LiAl3F12 (mp-13634) 0.7417 0.000 4
WO3 (mvc-5096) 0.4407 0.005 2
WO3 (mp-705411) 0.4147 0.004 2
WO3 (mp-32662) 0.4101 0.004 2
MnF3 (mp-556560) 0.3510 0.000 2
WO3 (mp-32777) 0.4431 0.005 2
CsTaCo(OF2)2 (mp-705413) 0.7320 0.000 5
TiNbTl(O2F)2 (mp-677378) 0.7325 0.039 5
TiTlWO5F (mp-690560) 0.6741 0.000 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

Two kinds of WO3 powders (referred to as WO3(PA) and WO3(C)) were prepared from W metal and H2O2. W metal powder (0.0226mol, Araido Material Co.) was completely dissolved in aqueous H2O2 (0.507mol, [...]
Two different procedures were used for preparation of hydrated zirconia. According to procedure 1, hydrated zirconia (denoted as HZ-1) was prepared by hydrolysis of 0.3M solution of zirconyl chloride [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition WO3.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
W: 6.2 eV
Pseudopotentials
VASP PAW: W_pv O
Final Energy/Atom
-7.5074 eV
Corrected Energy
-146.1143 eV
Uncorrected energy = -120.1183 eV Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV Composition-based energy adjustment (-4.438 eV/atom x 4.0 atoms) = -17.7520 eV Corrected energy = -146.1143 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)