Final Magnetic Moment0.930 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.024 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.679 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCrN |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
C (mp-48) | <0 0 1> | <1 0 0> | 31.6 |
C (mp-48) | <1 0 0> | <1 1 0> | 80.4 |
C (mp-48) | <1 0 1> | <1 1 0> | 80.4 |
C (mp-48) | <1 1 0> | <1 0 0> | 132.7 |
C (mp-48) | <1 1 1> | <1 1 0> | 134.1 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 76.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 284.4 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 294.9 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 241.3 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 107.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 31.6 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 158.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 31.6 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 98.3 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 53.6 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 208.0 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 32.8 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 142.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 139.0 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 142.3 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 80.4 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 321.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 82.2 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 169.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 31.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 126.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 208.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 316.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 221.2 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 175.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 82.2 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 107.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 139.0 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 35.7 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 221.2 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 208.0 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 208.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 31.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 143.0 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 98.3 |
InP (mp-20351) | <1 1 1> | <1 1 1> | 175.1 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 21.9 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 116.2 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 107.2 |
CdWO4 (mp-19387) | <0 1 0> | <1 1 0> | 223.4 |
CdWO4 (mp-19387) | <0 1 1> | <1 0 0> | 208.5 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 0> | 160.9 |
CdWO4 (mp-19387) | <1 1 1> | <1 0 0> | 208.5 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 76.6 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 10.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlVFeCo (mp-1008530) | 0.0000 | 0.029 | 4 |
TiFeCoSi (mp-998971) | 0.0000 | 0.029 | 4 |
TiGaFeCo (mp-998964) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
MnFeCoGe (mp-1018024) | 0.0000 | 0.007 | 4 |
BePd (mp-11274) | 0.0000 | 0.000 | 2 |
EuHg (mp-11375) | 0.0000 | 0.000 | 2 |
PuAs (mp-20773) | 0.0000 | 0.207 | 2 |
ScAg (mp-11237) | 0.0000 | 0.000 | 2 |
DyTh (mp-20379) | 0.0000 | 0.147 | 2 |
LiHo2Ir (mp-867913) | 0.0000 | 0.000 | 3 |
LiZn2Ir (mp-867253) | 0.0000 | 0.000 | 3 |
Sc2MnC (mp-999257) | 0.0000 | 0.874 | 3 |
FeTc2Cl (mp-631425) | 0.0000 | 1.059 | 3 |
GaSiRu2 (mp-865615) | 0.0000 | 0.000 | 3 |
Ge (mp-998883) | 0.0000 | 0.339 | 1 |
Ni (mp-1008728) | 0.0000 | 0.096 | 1 |
Si (mp-1014212) | 0.0000 | 0.525 | 1 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Al (mp-998860) | 0.0000 | 0.092 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cr_pv N |
Final Energy/Atom-8.8270 eV |
Corrected Energy-17.6540 eV
-17.6540 eV = -17.6540 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)