Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.644 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.080 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.00 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZnF2 + BiF3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 1> | 288.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 295.5 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 320.4 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 128.1 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 285.0 |
GaN (mp-804) | <1 1 0> | <1 1 -1> | 287.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 177.3 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 277.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 285.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 256.3 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 285.0 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 211.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 177.3 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 320.4 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 255.2 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 213.7 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 236.4 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 142.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 277.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 295.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 59.1 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 285.0 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 256.3 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 105.8 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 285.0 |
Te2Mo (mp-602) | <0 0 1> | <1 1 -1> | 287.5 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 256.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 320.4 |
BN (mp-984) | <0 0 1> | <0 1 1> | 288.3 |
BN (mp-984) | <1 0 0> | <0 1 0> | 285.0 |
BN (mp-984) | <1 0 1> | <1 1 0> | 277.7 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 -1> | 192.2 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 1> | 211.7 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 -1> | 128.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 285.0 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 192.2 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 256.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 -1> | 191.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 177.3 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 277.7 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 285.0 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 285.0 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 236.4 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 236.4 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 295.5 |
SiC (mp-7631) | <1 0 1> | <0 1 0> | 142.5 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 1> | 211.7 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 295.5 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 71.2 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 295.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MgBiF5 (mvc-15870) | 0.5188 | 0.101 | 3 |
MgSnF5 (mvc-15867) | 0.4314 | 0.182 | 3 |
MgWF5 (mvc-14224) | 0.5432 | 0.109 | 3 |
ZnBiF5 (mvc-16217) | 0.0992 | 0.080 | 3 |
MgAgF5 (mvc-3410) | 0.5612 | 0.109 | 3 |
Mg2SnWO6 (mvc-5015) | 0.7437 | 0.156 | 4 |
LiV(OF)2 (mp-772395) | 0.7291 | 0.004 | 4 |
NaV(OF)2 (mp-18953) | 0.6210 | 0.000 | 4 |
LiVOF3 (mp-765230) | 0.7228 | 0.004 | 4 |
V2Ni(TeO5)2 (mp-566026) | 0.7198 | 0.013 | 4 |
Hg12SbBr(ClO3)2 (mp-642625) | 0.6997 | 0.032 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zn Bi F |
Final Energy/Atom-4.3943 eV |
Corrected Energy-61.5198 eV
-61.5198 eV = -61.5198 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)