Final Magnetic Moment0.016 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.032 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.640 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe2O3 + Al2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 361.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 192.9 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 109.0 |
GaAs (mp-2534) | <1 1 0> | <1 1 1> | 285.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 192.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 289.4 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 109.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 265.3 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 43.6 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 103.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 120.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 290.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 313.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 192.9 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 218.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 290.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 261.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 1> | 285.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 192.9 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 218.1 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 174.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 120.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 109.0 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 349.0 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 218.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 313.5 |
ZnSe (mp-1190) | <1 1 0> | <1 1 1> | 285.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 217.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 192.9 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 174.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 363.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 289.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 181.7 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 155.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 144.7 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 51.7 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 109.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 120.6 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 131.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 217.1 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 206.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 144.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 144.7 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 305.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 217.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 217.1 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 289.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 217.1 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 109.0 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 145.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MgWO3 (mvc-5026) | 0.2508 | 0.185 | 3 |
Li3MnF6 (mp-764288) | 0.2461 | 0.188 | 3 |
MgBiO3 (mvc-15669) | 0.1590 | 0.124 | 3 |
AlCrO3 (mvc-14409) | 0.2013 | 0.376 | 3 |
LiFeF3 (mp-776189) | 0.2120 | 0.535 | 3 |
Zn2MoWO6 (mvc-5052) | 0.2583 | 0.038 | 4 |
VZn2WO6 (mvc-5045) | 0.2509 | 0.072 | 4 |
TiZn2WO6 (mvc-5017) | 0.2778 | 0.090 | 4 |
Zn2SnSbO6 (mvc-3962) | 0.2667 | 0.134 | 4 |
Zn2SbMoO6 (mvc-13704) | 0.2663 | 0.143 | 4 |
V3O5 (mp-714914) | 0.5190 | 0.004 | 2 |
V3O5 (mp-714911) | 0.5238 | 0.003 | 2 |
V3O5 (mp-542441) | 0.5244 | 0.029 | 2 |
Ti4O7 (mp-12205) | 0.5382 | 0.005 | 2 |
Ti4O7 (mp-558097) | 0.5390 | 0.005 | 2 |
Li4CrSb(WO6)2 (mp-764950) | 0.5146 | 0.036 | 5 |
Li4CrTe2WO12 (mp-775509) | 0.5011 | 0.109 | 5 |
Li4FeTe2WO12 (mp-775176) | 0.5074 | 0.208 | 5 |
Li4CrSb(TeO6)2 (mp-781050) | 0.5117 | 0.048 | 5 |
Li4FeSb(WO6)2 (mp-767012) | 0.5185 | 0.033 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Al Fe_pv O |
Final Energy/Atom-6.4757 eV |
Corrected Energy-148.8734 eV
-148.8734 eV = -129.5139 eV (uncorrected energy) - 10.9320 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)