Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.626 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.65 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.893 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI42d [122] |
HallI 4 2bw |
Point Group42m |
Crystal Systemtetragonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
C (mp-66) | <1 0 0> | <0 0 1> | 0.005 | 63.7 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 0.012 | 63.7 |
MgF2 (mp-1249) | <1 0 1> | <0 0 1> | 0.014 | 159.2 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 0.017 | 31.8 |
InP (mp-20351) | <1 0 0> | <1 1 1> | 0.024 | 283.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 0.031 | 159.2 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 0.032 | 63.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 0.034 | 63.7 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 0.038 | 188.6 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <0 0 1> | 0.038 | 159.2 |
GdScO3 (mp-5690) | <0 1 0> | <1 1 0> | 0.039 | 88.9 |
ZnO (mp-2133) | <1 1 1> | <1 0 0> | 0.041 | 62.9 |
ZnO (mp-2133) | <1 1 0> | <1 0 1> | 0.048 | 211.4 |
TiO2 (mp-2657) | <0 0 1> | <1 1 1> | 0.051 | 283.3 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 0.055 | 251.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 0.062 | 222.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 0.064 | 159.2 |
SrTiO3 (mp-4651) | <1 0 0> | <1 1 0> | 0.065 | 88.9 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 0.065 | 266.8 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 0> | 0.074 | 266.8 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 0.076 | 159.2 |
C (mp-48) | <0 0 1> | <1 0 1> | 0.077 | 211.4 |
MgF2 (mp-1249) | <0 0 1> | <1 1 1> | 0.082 | 283.3 |
YAlO3 (mp-3792) | <1 1 0> | <1 1 1> | 0.097 | 283.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 0.106 | 318.4 |
Al (mp-134) | <1 1 1> | <0 0 1> | 0.108 | 222.9 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 0.113 | 251.5 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 0.122 | 286.6 |
Au (mp-81) | <1 0 0> | <0 0 1> | 0.124 | 159.2 |
Au (mp-81) | <1 1 0> | <1 1 0> | 0.126 | 266.8 |
LaF3 (mp-905) | <1 1 0> | <1 0 1> | 0.138 | 281.9 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 0.141 | 31.8 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 1> | 0.144 | 70.5 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 0.148 | 31.8 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 0.154 | 314.4 |
TbScO3 (mp-31119) | <0 1 0> | <1 1 0> | 0.159 | 88.9 |
NaCl (mp-22862) | <1 1 1> | <1 1 1> | 0.169 | 283.3 |
WS2 (mp-224) | <1 1 1> | <0 0 1> | 0.169 | 159.2 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 0.176 | 251.5 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 0.177 | 283.3 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 1> | 0.178 | 94.4 |
PbS (mp-21276) | <1 0 0> | <1 1 1> | 0.178 | 283.3 |
BN (mp-984) | <1 0 1> | <1 1 0> | 0.179 | 177.8 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 0.180 | 70.5 |
WS2 (mp-224) | <1 1 0> | <0 0 1> | 0.181 | 159.2 |
C (mp-48) | <1 0 1> | <0 0 1> | 0.186 | 254.7 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 0.193 | 62.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 0.194 | 191.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 0.195 | 62.9 |
CsI (mp-614603) | <1 1 0> | <1 1 0> | 0.195 | 88.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
86 | 49 | 52 | 0 | 0 | 0 |
49 | 86 | 52 | 0 | 0 | 0 |
52 | 52 | 88 | 0 | 0 | 0 |
0 | 0 | 0 | 39 | 0 | 0 |
0 | 0 | 0 | 0 | 39 | 0 |
0 | 0 | 0 | 0 | 0 | 38 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
20.1 | -6.6 | -7.9 | 0 | 0 | 0 |
-6.6 | 20.1 | -7.9 | 0 | 0 | 0 |
-7.9 | -7.9 | 20.7 | 0 | 0 | 0 |
0 | 0 | 0 | 25.6 | 0 | 0 |
0 | 0 | 0 | 0 | 25.6 | 0 |
0 | 0 | 0 | 0 | 0 | 26.2 |
Shear Modulus GV30 GPa |
Bulk Modulus KV63 GPa |
Shear Modulus GR26 GPa |
Bulk Modulus KR63 GPa |
Shear Modulus GVRH28 GPa |
Bulk Modulus KVRH63 GPa |
Elastic Anisotropy0.75 |
Poisson's Ratio0.30 |
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.04272 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.04272 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.04074 |
Piezoelectric Modulus ‖eij‖max0.04272 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
1.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
8.09 | 0.00 | 0.00 |
0.00 | 8.09 | 0.00 |
0.00 | 0.00 | 8.06 |
Dielectric Tensor εij (total) |
||
---|---|---|
10.02 | 0.00 | 0.00 |
0.00 | 10.02 | 0.00 |
0.00 | 0.00 | 10.34 |
Polycrystalline dielectric constant
εpoly∞
8.08
|
Polycrystalline dielectric constant
εpoly
10.13
|
Refractive Index n2.84 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnGeAs2 (mp-4008) | 0.0106 | 0.000 | 3 |
MgSnP2 (mp-1009083) | 0.0102 | 0.011 | 3 |
CdSnSb2 (mp-10063) | 0.0032 | 0.000 | 3 |
ZnGeP2 (mp-4524) | 0.0190 | 0.000 | 3 |
GaCuS2 (mp-5238) | 0.0089 | 0.000 | 3 |
FeCu2GeS4 (mp-917359) | 0.0156 | 0.185 | 4 |
CoCu2GeS4 (mp-6498) | 0.0294 | 0.055 | 4 |
CoCu2GeS4 (mp-560428) | 0.0371 | 0.055 | 4 |
FeCu2GeS4 (mp-22053) | 0.0087 | 0.185 | 4 |
FeCu2GeSe4 (mp-1087471) | 0.0731 | 0.036 | 4 |
ZrO (mp-33088) | 0.0253 | 0.424 | 2 |
CoO (mp-557513) | 0.0253 | 0.000 | 2 |
ZnNi (mp-567903) | 0.0253 | 1.083 | 2 |
CuS (mp-760381) | 0.0234 | 0.013 | 2 |
CoO (mp-24864) | 0.0253 | 0.000 | 2 |
Si (mp-149) | 0.0253 | 0.000 | 1 |
Sn (mp-117) | 0.0253 | 0.000 | 1 |
C (mp-66) | 0.0253 | 0.136 | 1 |
Ge (mp-32) | 0.0253 | 0.000 | 1 |
Se (mp-12771) | 0.0253 | 0.514 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Al Cu_pv Se |
Final Energy/Atom-4.3347 eV |
Corrected Energy-34.6773 eV
-34.6773 eV = -34.6773 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)