material

AlFeF5

ID:

mp-28901


Tags: Iron aluminium fluoride

Material Details

Final Magnetic Moment
4.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-3.401 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.010 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.42 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
FeF2 + AlF3
Band Gap
3.408 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Immm [71]
Hall
-I 2 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 78012 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgF2 (mp-1249) <0 0 1> <1 0 1> 0.005 265.0
Cu (mp-30) <1 0 0> <0 0 1> 0.009 91.2
Te2W (mp-22693) <1 1 1> <0 0 1> 0.017 114.0
LiGaO2 (mp-5854) <1 0 1> <1 1 1> 0.018 178.9
BaF2 (mp-1029) <1 0 0> <1 0 1> 0.020 159.0
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.026 205.1
LaF3 (mp-905) <0 0 1> <0 0 1> 0.027 45.6
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.027 182.3
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.027 182.3
BN (mp-984) <0 0 1> <0 0 1> 0.027 136.7
LiF (mp-1138) <1 1 1> <1 0 1> 0.028 318.0
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.031 45.6
CdWO4 (mp-19387) <1 1 0> <0 0 1> 0.031 205.1
YVO4 (mp-19133) <1 0 0> <0 0 1> 0.045 45.6
AlN (mp-661) <0 0 1> <0 0 1> 0.046 68.4
TiO2 (mp-390) <0 0 1> <1 0 0> 0.046 143.5
DyScO3 (mp-31120) <0 1 1> <0 1 1> 0.048 106.8
InP (mp-20351) <1 1 0> <0 1 0> 0.055 300.6
AlN (mp-661) <1 0 1> <1 0 0> 0.060 143.5
TiO2 (mp-390) <1 0 1> <1 0 0> 0.060 239.2
MgF2 (mp-1249) <1 0 0> <1 0 1> 0.065 159.0
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.067 182.3
AlN (mp-661) <1 0 0> <1 0 1> 0.068 159.0
TePb (mp-19717) <1 1 0> <0 1 0> 0.074 246.0
CdS (mp-672) <0 0 1> <0 0 1> 0.077 45.6
InAs (mp-20305) <1 1 1> <0 1 0> 0.078 327.9
ZnTe (mp-2176) <1 1 1> <0 1 0> 0.088 327.9
CdWO4 (mp-19387) <0 0 1> <0 1 0> 0.090 273.3
GdScO3 (mp-5690) <1 0 1> <0 1 1> 0.092 284.7
GaSe (mp-1943) <1 0 1> <1 1 0> 0.098 275.5
LaAlO3 (mp-2920) <1 1 0> <0 1 0> 0.099 246.0
Ag (mp-124) <1 1 0> <0 1 0> 0.102 218.6
InP (mp-20351) <1 1 1> <0 0 1> 0.106 182.3
TbScO3 (mp-31119) <0 1 1> <0 1 1> 0.110 106.8
KCl (mp-23193) <1 1 0> <0 0 1> 0.110 114.0
NdGaO3 (mp-3196) <1 0 1> <0 0 1> 0.110 159.5
AlN (mp-661) <1 1 1> <1 0 1> 0.111 318.0
NdGaO3 (mp-3196) <0 1 0> <0 0 1> 0.113 296.3
KP(HO2)2 (mp-23959) <1 1 0> <0 0 1> 0.116 136.7
LiGaO2 (mp-5854) <0 1 1> <1 0 1> 0.122 212.0
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.125 95.7
CdTe (mp-406) <1 1 0> <0 1 0> 0.141 246.0
GaTe (mp-542812) <0 0 1> <0 0 1> 0.142 227.9
BaTiO3 (mp-5986) <1 1 0> <1 0 1> 0.142 212.0
CaCO3 (mp-3953) <1 0 1> <0 1 0> 0.145 273.3
BaTiO3 (mp-5986) <1 0 1> <1 1 0> 0.147 275.5
BaTiO3 (mp-5986) <1 0 0> <1 0 1> 0.147 265.0
InSb (mp-20012) <1 1 0> <0 1 0> 0.161 246.0
ZrO2 (mp-2858) <0 1 1> <1 0 0> 0.165 239.2
C (mp-66) <1 0 0> <0 0 1> 0.166 91.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
2.11 -0.00 0.00
-0.00 2.13 -0.00
0.00 -0.00 2.14
Dielectric Tensor εij (total)
7.55 -0.00 0.00
-0.00 4.83 -0.00
0.00 -0.00 7.56
Polycrystalline dielectric constant εpoly
(electronic contribution)
2.13
Polycrystalline dielectric constant εpoly
(total)
6.65
Refractive Index n
1.46
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
W3O7 (mvc-9357) 0.7206 0.097 2
Ta2O5 (mp-554867) 0.6564 0.319 2
IrO3 (mp-1022963) 0.6584 0.044 2
P2O5 (mp-990076) 0.6219 0.677 2
MnAlF5 (mvc-14725) 0.0720 0.009 3
TiAlF5 (mvc-13886) 0.0734 0.139 3
AlCrF5 (mvc-15887) 0.0879 0.010 3
AlFeF5 (mvc-16231) 0.0081 0.010 3
AlCoF5 (mvc-15886) 0.0660 0.049 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Fe: 5.3 eV
Pseudopotentials
VASP PAW: Al Fe_pv F
Final Energy/Atom
-5.7705 eV
Corrected Energy
-43.1264 eV
-43.1264 eV = -40.3934 eV (uncorrected energy) - 2.7330 eV (MP Advanced Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 78012
Submitted by
User remarks:
  • Iron aluminium fluoride