Final Magnetic Moment7.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.148 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.165 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCo3O4 + CoO + Y2O3 |
Band Gap0.634 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImma [74] |
Hall-I 2b 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 197.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 279.5 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 156.7 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 159.7 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 68.3 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 131.5 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 313.4 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 261.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 328.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 319.4 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 152.3 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 159.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 199.7 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 156.7 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 328.8 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 328.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 359.4 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 52.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 359.4 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 156.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 257.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 319.4 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 228.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 261.2 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 166.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 119.8 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 76.1 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 328.8 |
Te2W (mp-22693) | <1 0 1> | <1 0 1> | 204.9 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 261.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 208.9 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 239.6 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 68.3 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 166.2 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 119.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 359.4 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 208.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 68.3 |
Te2W (mp-22693) | <0 1 1> | <1 1 1> | 171.9 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 199.7 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 65.8 |
Te2Mo (mp-602) | <1 0 0> | <0 1 1> | 328.8 |
Te2Mo (mp-602) | <1 0 1> | <0 1 1> | 328.8 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 279.5 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 263.0 |
Ag (mp-124) | <1 1 0> | <1 1 1> | 171.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 199.7 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 277.0 |
BN (mp-984) | <0 0 1> | <0 1 0> | 261.2 |
BN (mp-984) | <1 0 0> | <1 0 0> | 332.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YV2O4 (mvc-16805) | 0.1163 | 0.145 | 3 |
Y(NiO2)2 (mvc-16809) | 0.1042 | 0.340 | 3 |
Y(FeO2)2 (mvc-16797) | 0.1156 | 0.410 | 3 |
Li(CrS2)2 (mvc-16755) | 0.1481 | 0.158 | 3 |
LiMnNbO4 (mp-861574) | 0.1854 | 0.017 | 4 |
LiNbCoO4 (mp-772384) | 0.1734 | 0.143 | 4 |
LiNbFeO4 (mp-772339) | 0.1966 | 0.005 | 4 |
LiNbNiO4 (mp-779181) | 0.1771 | 0.018 | 4 |
LiNbVO4 (mp-761817) | 0.1925 | 0.034 | 4 |
Fe3O4 (mp-715491) | 0.2091 | 0.017 | 2 |
Fe3O4 (mp-567124) | 0.2416 | 0.017 | 2 |
Fe3O4 (mp-650112) | 0.2475 | 0.060 | 2 |
Fe3O4 (mp-31770) | 0.1995 | 0.017 | 2 |
Fe3O4 (mp-716052) | 0.2527 | 0.781 | 2 |
Li4Cr3Ni3(TeO8)2 (mp-761407) | 0.3187 | 0.179 | 5 |
Li4Mn3Fe3(SbO8)2 (mp-775013) | 0.3312 | 0.005 | 5 |
Li4Fe3Ni3(TeO8)2 (mp-773382) | 0.3003 | 0.197 | 5 |
Li4Cr3Fe3(SbO8)2 (mp-771925) | 0.3376 | 0.871 | 5 |
Li4Fe3Co3(TeO8)2 (mp-849468) | 0.3167 | 0.067 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.6056 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.5936 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6015 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6018 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6050 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Y_sv Co O |
Final Energy/Atom-6.9931 eV |
Corrected Energy-111.0172 eV
-111.0172 eV = -97.9029 eV (uncorrected energy) - 7.4960 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)