Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.561 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.207 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.30 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAlV2O4 |
Band Gap0.452 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImma [74] |
Hall-I 2b 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 106.0 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 241.8 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 290.2 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 193.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 211.9 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 278.7 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 239.6 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 48.4 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 317.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 211.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 317.9 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 179.7 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 241.8 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 184.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 150.4 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 145.1 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 239.6 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 48.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 96.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 141.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 282.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 317.9 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 150.4 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 106.0 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 241.8 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 250.7 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 234.3 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 59.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 239.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 70.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 176.6 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 338.6 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 48.4 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 290.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 306.7 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 193.5 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 184.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 176.6 |
Te2Mo (mp-602) | <1 1 1> | <1 0 1> | 184.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 35.3 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 48.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 119.8 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 179.7 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 59.9 |
BN (mp-984) | <0 0 1> | <0 1 0> | 241.8 |
BN (mp-984) | <1 0 0> | <1 0 1> | 306.7 |
BN (mp-984) | <1 0 1> | <0 1 0> | 241.8 |
BN (mp-984) | <1 1 0> | <0 1 1> | 239.6 |
BN (mp-984) | <1 1 1> | <0 1 0> | 241.8 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 1> | 299.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(CoO2)2 (mp-763702) | 0.2007 | 0.071 | 3 |
LiV2O4 (mp-771663) | 0.2107 | 0.091 | 3 |
Ca(CrS2)2 (mvc-16771) | 0.2401 | 0.113 | 3 |
CaCr2O4 (mvc-16821) | 0.2417 | 0.108 | 3 |
Li(CoO2)2 (mvc-16808) | 0.2077 | 0.032 | 3 |
Li2TiCr3O8 (mp-780807) | 0.2260 | 0.092 | 4 |
Li2MnCr3O8 (mp-780543) | 0.1900 | 0.094 | 4 |
LiVCrO4 (mp-853248) | 0.1644 | 0.088 | 4 |
LiTiVO4 (mp-763509) | 0.1497 | 0.096 | 4 |
Li2V3CrO8 (mp-781740) | 0.2271 | 0.082 | 4 |
Ni3O4 (mp-714961) | 0.4892 | 0.000 | 2 |
Fe3O4 (mp-715614) | 0.4029 | 0.466 | 2 |
Fe3O4 (mp-612405) | 0.4780 | 0.175 | 2 |
Ni3O4 (mp-656887) | 0.4934 | 0.000 | 2 |
Zr3S4 (mp-684749) | 0.4999 | 0.000 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Al V_pv O |
Final Energy/Atom-7.6373 eV |
Corrected Energy-119.2683 eV
-119.2683 eV = -106.9220 eV (uncorrected energy) - 6.7280 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)