Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.707 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.158 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu2O + Y3SbO7 + CuO + SbO2 |
Band Gap0.056 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIm3 [204] |
Hall-I 2 2 3 |
Point Groupm3 |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 313.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 313.6 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 313.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 177.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 250.9 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 313.6 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 177.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 88.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 88.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 62.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 313.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 313.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 313.6 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 108.6 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 313.6 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 250.9 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 250.9 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 177.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 313.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 313.6 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 313.6 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 177.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 313.6 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 266.1 |
BN (mp-984) | <0 0 1> | <1 0 0> | 313.6 |
BN (mp-984) | <1 0 0> | <1 1 0> | 177.4 |
BN (mp-984) | <1 1 0> | <1 0 0> | 313.6 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 313.6 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 313.6 |
GdScO3 (mp-5690) | <0 1 0> | <1 1 0> | 88.7 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 62.7 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 313.6 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 250.9 |
Al (mp-134) | <1 1 0> | <1 0 0> | 313.6 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 188.2 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 62.7 |
GaP (mp-2490) | <1 1 0> | <1 1 0> | 88.7 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 313.6 |
TbScO3 (mp-31119) | <0 1 0> | <1 1 0> | 88.7 |
TbScO3 (mp-31119) | <1 0 0> | <1 1 0> | 88.7 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 250.9 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 313.6 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 177.4 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 0> | 266.1 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 188.2 |
NdGaO3 (mp-3196) | <0 1 0> | <1 1 0> | 88.7 |
NdGaO3 (mp-3196) | <1 0 0> | <1 1 0> | 88.7 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 313.6 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 62.7 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 188.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiMn7O12 (mp-769733) | 0.4431 | 0.061 | 3 |
Li3CuF6 (mp-760812) | 0.3670 | 0.045 | 3 |
PrMn7O12 (mp-19354) | 0.4179 | 0.022 | 3 |
YCu7O12 (mvc-1832) | 0.3140 | 0.000 | 3 |
AlCu7O12 (mvc-1846) | 0.1358 | 0.209 | 3 |
AlCu3(SnO3)4 (mvc-1888) | 0.1658 | 0.368 | 4 |
YCu3(SnO3)4 (mvc-1875) | 0.1203 | 0.123 | 4 |
AlCo4(CuO4)3 (mvc-2124) | 0.1723 | 0.235 | 4 |
Mn4Al(CuO4)3 (mvc-2132) | 0.1108 | 0.243 | 4 |
YCu3(MoO3)4 (mvc-2235) | 0.1726 | 0.226 | 4 |
CaCr2Cu3(SbO6)2 (mp-510534) | 0.3896 | 0.060 | 5 |
CaNb2Ga2(CuO4)3 (mp-686705) | 0.3898 | 0.111 | 5 |
CaGa2Cu3(SbO6)2 (mp-41331) | 0.3872 | 0.080 | 5 |
NdTi3Fe(CuO4)3 (mp-690601) | 0.3680 | 0.046 | 5 |
NdTi3Fe(CuO4)3 (mp-39888) | 0.3694 | 0.046 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Y_sv Cu_pv Sb O |
Final Energy/Atom-6.0187 eV |
Corrected Energy-128.8009 eV
-128.8009 eV = -120.3734 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)