Final Magnetic Moment6.321 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.614 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.165 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSrCr2O4 + Tl2O + SrO + Y2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/mmm [123] |
Hall-P 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 75.2 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 75.2 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 345.7 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 206.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 75.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 240.5 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 246.9 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 139.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 225.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 30.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 206.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 45.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 165.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 135.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 75.2 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 148.2 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 142.9 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 214.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 195.4 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 206.5 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 285.8 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 139.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 240.5 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 139.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 225.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 135.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 135.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 279.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 255.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 270.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 255.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 285.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 75.2 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 206.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 255.5 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 206.5 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 246.9 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 300.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 135.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 255.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 345.7 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 206.5 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 330.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 270.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 255.5 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 330.7 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 300.6 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 258.1 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 309.7 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 270.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Sr_sv Y_sv Tl_d Cr_pv O |
Final Energy/Atom-7.0146 eV |
Corrected Energy-100.1321 eV
-100.1321 eV = -91.1901 eV (uncorrected energy) - 4.9160 eV (MP Anion Correction) - 4.0260 eV (MP Advanced Correction)
|