Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.755 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.028 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSrZn2(PO4)2 + SrMn2(PO4)2 |
Band Gap3.216 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 -1 0> | 286.3 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 155.2 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 125.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 192.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 192.4 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 227.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 269.4 |
AlN (mp-661) | <1 1 1> | <0 1 -1> | 203.5 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 155.2 |
CeO2 (mp-20194) | <1 1 0> | <0 1 -1> | 305.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 115.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 115.5 |
GaN (mp-804) | <1 1 0> | <0 1 -1> | 203.5 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 191.8 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 269.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 -1> | 305.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 -1> | 163.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 230.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 310.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 313.2 |
ZnSe (mp-1190) | <1 1 0> | <1 -1 0> | 143.1 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 250.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 269.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 115.5 |
Te2W (mp-22693) | <0 0 1> | <0 1 -1> | 203.5 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 223.2 |
Te2Mo (mp-602) | <0 0 1> | <1 -1 1> | 239.1 |
Ag (mp-124) | <1 0 0> | <1 1 -1> | 245.1 |
Ag (mp-124) | <1 1 0> | <0 1 -1> | 305.3 |
BN (mp-984) | <0 0 1> | <1 1 1> | 223.2 |
BN (mp-984) | <1 0 1> | <0 1 0> | 258.7 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 115.5 |
MoS2 (mp-1434) | <1 1 1> | <0 0 1> | 115.5 |
Al (mp-134) | <1 1 0> | <0 0 1> | 115.5 |
LiGaO2 (mp-5854) | <0 1 0> | <1 -1 -1> | 165.6 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 1> | 246.0 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 1> | 246.0 |
CdTe (mp-406) | <1 0 0> | <1 1 1> | 223.2 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 125.3 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 192.4 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 258.7 |
MgO (mp-1265) | <1 1 1> | <0 1 -1> | 254.4 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 230.9 |
TiO2 (mp-2657) | <1 0 0> | <1 0 -1> | 191.8 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 313.2 |
TiO2 (mp-2657) | <1 1 1> | <0 1 -1> | 203.5 |
C (mp-66) | <1 1 0> | <0 1 0> | 258.7 |
C (mp-66) | <1 1 1> | <0 1 0> | 258.7 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 230.9 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 -1> | 305.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LaTcN3 (mp-989619) | 0.5944 | 0.000 | 3 |
Li2Cr2O7 (mp-770745) | 0.5595 | 0.068 | 3 |
Na2Cr2O7 (mp-704459) | 0.5984 | 0.000 | 3 |
Ca5Ge3O11 (mp-774105) | 0.5800 | 0.016 | 3 |
Na2Mo2O7 (mp-25774) | 0.5854 | 0.000 | 3 |
Na4MoS3O14 (mp-565395) | 0.4667 | 0.000 | 4 |
MgTi2(PO4)2 (mvc-9555) | 0.4953 | 0.338 | 4 |
CaV2(PO4)2 (mvc-9882) | 0.5090 | 0.047 | 4 |
ZnAg2P2O9 (mvc-9821) | 0.5153 | 0.105 | 4 |
MgAg2P2O9 (mvc-9823) | 0.4932 | 0.107 | 4 |
SrTiZn(PO4)2 (mvc-2665) | 0.1806 | 0.170 | 5 |
SrMgMn(PO4)2 (mvc-2987) | 0.1583 | 0.019 | 5 |
SrMgCo(PO4)2 (mvc-2989) | 0.2150 | 0.024 | 5 |
SrZnCo(PO4)2 (mvc-2988) | 0.2117 | 0.034 | 5 |
SrZnFe(PO4)2 (mvc-3016) | 0.1377 | 0.023 | 5 |
Na3Zn4P4H4NO16 (mp-772852) | 0.5945 | 0.005 | 6 |
NaLiMn2Fe4(PO4)6 (mp-777193) | 0.6203 | 0.021 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Sr_sv Mn_pv Zn P O |
Final Energy/Atom-7.0031 eV |
Corrected Energy-393.3602 eV
-393.3602 eV = -364.1635 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)