Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.817 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.010 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.80 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSr2Ni(PO4)2 + Ni3(PO4)2 + Mg3(PO4)2 |
Band Gap3.984 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 150.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 112.8 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 150.4 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 250.6 |
GaN (mp-804) | <1 1 0> | <0 1 -1> | 197.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 -1> | 197.6 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 247.2 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 260.6 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 250.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 300.8 |
ZnSe (mp-1190) | <1 1 1> | <0 1 1> | 294.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 263.1 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 309.0 |
CdS (mp-672) | <1 1 1> | <1 -1 -1> | 160.2 |
LiF (mp-1138) | <1 0 0> | <1 -1 1> | 230.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 112.8 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 309.0 |
Te2W (mp-22693) | <1 1 1> | <0 1 1> | 220.7 |
TePb (mp-19717) | <1 0 0> | <1 1 1> | 216.0 |
Te2Mo (mp-602) | <1 0 1> | <0 1 1> | 220.7 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 294.2 |
GaSe (mp-1943) | <1 1 1> | <1 -1 -1> | 240.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 300.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 300.7 |
BN (mp-984) | <1 0 1> | <1 -1 0> | 206.6 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 120.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 1> | 316.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 112.8 |
MoS2 (mp-1434) | <1 0 0> | <0 1 -1> | 197.6 |
Al (mp-134) | <1 0 0> | <1 -1 1> | 230.3 |
Al (mp-134) | <1 1 0> | <0 0 1> | 112.8 |
Al (mp-134) | <1 1 1> | <1 0 -1> | 309.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 -1> | 197.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 300.7 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 -1> | 309.0 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 241.0 |
LiGaO2 (mp-5854) | <1 0 1> | <1 -1 0> | 137.7 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 1> | 237.5 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 1> | 220.7 |
CdTe (mp-406) | <1 0 0> | <1 1 1> | 216.0 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 187.9 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 225.5 |
TeO2 (mp-2125) | <0 1 0> | <0 1 -1> | 197.6 |
TeO2 (mp-2125) | <0 1 1> | <0 1 0> | 150.4 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 300.7 |
SiC (mp-7631) | <0 0 1> | <1 -1 -1> | 240.3 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 187.9 |
SiC (mp-7631) | <1 1 1> | <0 1 -1> | 247.0 |
LiTaO3 (mp-3666) | <1 1 0> | <0 1 -1> | 247.0 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 250.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La2SiO5 (mp-771045) | 0.5969 | 0.050 | 3 |
Li2Cr2O7 (mp-770745) | 0.5183 | 0.068 | 3 |
Ca5Ge3O11 (mp-774105) | 0.5948 | 0.016 | 3 |
Na2Mo2O7 (mp-25774) | 0.5304 | 0.000 | 3 |
In2PO5 (mp-31232) | 0.5443 | 0.000 | 3 |
Li4Ni7(PO4)6 (mp-861539) | 0.4561 | 0.063 | 4 |
LiMn2(PO4)2 (mp-771366) | 0.4722 | 0.036 | 4 |
SrNi2(PO4)2 (mp-19647) | 0.2703 | 0.003 | 4 |
Na4Ni7(PO4)6 (mp-19470) | 0.4720 | 0.008 | 4 |
CaV2(PO4)2 (mvc-9882) | 0.4110 | 0.047 | 4 |
SrZnNi(PO4)2 (mvc-16452) | 0.2668 | 0.017 | 5 |
SrMgMn(PO4)2 (mvc-2987) | 0.3058 | 0.019 | 5 |
SrMgCo(PO4)2 (mvc-2989) | 0.2019 | 0.024 | 5 |
SrZnCo(PO4)2 (mvc-2988) | 0.3010 | 0.034 | 5 |
SrMgV(PO4)2 (mvc-2997) | 0.1529 | 0.026 | 5 |
Na2Gd2MgSi4(O6F)2 (mp-557538) | 0.6667 | 0.000 | 6 |
Na3Zn4P4H4NO16 (mp-772852) | 0.6397 | 0.005 | 6 |
NaLiMn2Fe4(PO4)6 (mp-777193) | 0.6122 | 0.021 | 6 |
Li4Mn3NbCr2(PO4)6 (mp-776566) | 0.7075 | 0.100 | 6 |
Li3Al3P3H2O14F (mp-695635) | 0.6770 | 0.003 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Sr_sv Mg_pv Ni_pv P O |
Final Energy/Atom-6.7938 eV |
Corrected Energy-192.2039 eV
-192.2039 eV = -176.6393 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 4.3280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)