Final Magnetic Moment0.815 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.251 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.167 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.65 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMgVO3 + V3O5 + Mg2Te3O8 + Te |
Band Gap0.125 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 296.5 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 296.5 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 176.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 162.1 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 296.5 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 296.5 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 296.5 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 296.5 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 176.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 197.6 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 176.0 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 137.3 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 296.5 |
CdTe (mp-406) | <1 1 1> | <1 0 0> | 296.5 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 98.8 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 296.5 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 137.3 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 296.5 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 296.5 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 296.5 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 296.5 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 -1> | 162.1 |
Si (mp-149) | <1 0 0> | <1 0 0> | 296.5 |
InSb (mp-20012) | <1 0 0> | <1 0 1> | 176.0 |
InSb (mp-20012) | <1 1 1> | <1 0 0> | 296.5 |
YAlO3 (mp-3792) | <0 1 1> | <1 0 0> | 98.8 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 0> | 98.8 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 0> | 197.6 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 98.8 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 137.3 |
TiO2 (mp-390) | <1 0 1> | <1 0 0> | 197.6 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 296.5 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 197.6 |
MgF2 (mp-1249) | <0 0 1> | <1 0 1> | 176.0 |
MgF2 (mp-1249) | <1 1 1> | <1 0 0> | 296.5 |
ZnO (mp-2133) | <1 1 0> | <1 0 0> | 296.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3VF6 (mp-622187) | 0.4585 | 0.143 | 3 |
Li3Mn2F7 (mp-764189) | 0.4829 | 0.051 | 3 |
Li3TiF6 (mp-21540) | 0.4270 | 0.000 | 3 |
Li3Fe2F7 (mp-777444) | 0.4796 | 0.480 | 3 |
Li3VF6 (mp-558578) | 0.4581 | 0.143 | 3 |
Li11V6O5F19 (mp-850254) | 0.4454 | 0.058 | 4 |
Li4Mn7O9F7 (mp-767099) | 0.4441 | 0.072 | 4 |
Zn4Cr5(TeO6)3 (mvc-3075) | 0.4867 | 0.277 | 4 |
Mg4Cr5(TeO6)3 (mvc-3078) | 0.4720 | 1.198 | 4 |
V5Zn4(TeO6)3 (mvc-3090) | 0.2380 | 0.096 | 4 |
V3O5 (mp-714914) | 0.6055 | 0.004 | 2 |
V3O5 (mp-622497) | 0.6073 | 0.004 | 2 |
V5O9 (mp-714932) | 0.6257 | 0.017 | 2 |
Ti4O7 (mp-12205) | 0.6386 | 0.005 | 2 |
Ti4O7 (mp-558097) | 0.6285 | 0.005 | 2 |
Li4FeSb(TeO6)2 (mp-780741) | 0.5528 | 0.040 | 5 |
Li4MnNb2WO12 (mp-771475) | 0.4777 | 0.046 | 5 |
Li4CrTe2WO12 (mp-775509) | 0.5085 | 0.109 | 5 |
Li4MnSb(WO6)2 (mp-779994) | 0.5508 | 0.041 | 5 |
Li4FeTe2WO12 (mp-775176) | 0.5062 | 0.208 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Mg_pv V_pv Te O |
Final Energy/Atom-6.5601 eV |
Corrected Energy-435.7103 eV
-435.7103 eV = -393.6079 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction) - 16.8200 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)