Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.694 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.065 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.63 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa3Fe2(SiO4)3 + Fe2O3 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 0 -1> | 197.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 329.1 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 329.1 |
GaN (mp-804) | <1 1 0> | <1 1 -1> | 234.6 |
GaN (mp-804) | <1 1 1> | <1 1 -1> | 156.4 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 248.2 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 211.1 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 288.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 337.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 109.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 109.6 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 263.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 234.4 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 109.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 337.7 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 168.9 |
CdS (mp-672) | <1 0 0> | <1 1 -1> | 234.6 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 248.2 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 288.9 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 150.1 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 253.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 248.2 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 310.2 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 295.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 175.8 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 109.6 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 197.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 -1> | 263.3 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 329.1 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 295.5 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 329.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 253.3 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 263.3 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 126.7 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 295.5 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 197.4 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 253.3 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 202.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 175.8 |
BN (mp-984) | <1 0 1> | <0 1 0> | 295.5 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 186.1 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 124.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 310.2 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 253.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 175.8 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 117.2 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 1> | 109.6 |
BN (mp-984) | <0 0 1> | <1 0 -1> | 65.8 |
BN (mp-984) | <1 0 0> | <0 1 1> | 288.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 168.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaGe2O5 (mp-554678) | 0.6275 | 0.014 | 3 |
Na2Mo2O5 (mp-1099875) | 0.6542 | 0.131 | 3 |
MnSi2O5 (mp-19351) | 0.3738 | 0.103 | 3 |
CaGe2O5 (mp-3707) | 0.3477 | 0.006 | 3 |
In2PO5 (mp-31232) | 0.6157 | 0.000 | 3 |
CaTiSiO5 (mp-6109) | 0.1250 | 0.000 | 4 |
CaTiGeO5 (mp-17784) | 0.2682 | 0.000 | 4 |
CaTiSiO5 (mp-6440) | 0.1663 | 0.000 | 4 |
NaVPO5 (mp-19291) | 0.3647 | 0.000 | 4 |
NaVAsO5 (mp-19621) | 0.3240 | 0.000 | 4 |
NaAlPO4F (mp-8678) | 0.3133 | 0.002 | 5 |
CaAlSiO4F (mp-6873) | 0.3108 | 0.029 | 5 |
NaAlAsO4F (mp-14395) | 0.4002 | 0.000 | 5 |
CaMgAsO4F (mp-558016) | 0.3788 | 0.000 | 5 |
CaMgAsO4F (mp-7035) | 0.3363 | 0.000 | 5 |
NaCa4TaTi4(SiO5)5 (mp-694049) | 0.2270 | 0.000 | 6 |
Ca10Ti8NbAl(SiO5)10 (mp-693409) | 0.2286 | 0.004 | 6 |
NaCa9Ti9Nb(SiO5)10 (mp-534850) | 0.2174 | 0.000 | 6 |
Ca5DyTi5Fe(SiO5)6 (mp-743624) | 0.2153 | 0.005 | 6 |
NaCa9TaTi9(SiO5)10 (mp-705502) | 0.2222 | 0.000 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Ca_sv Fe_pv Si O |
Final Energy/Atom-6.9940 eV |
Corrected Energy-124.3922 eV
-124.3922 eV = -111.9033 eV (uncorrected energy) - 7.0229 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)