Final Magnetic Moment0.015 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.598 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.279 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.20 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg(SbO2)2 + SiO2 + Mg2SiO4 |
Band Gap2.807 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIa3d [230] |
Hall-I 4bd 2c 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 152.4 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 152.4 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 152.4 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 152.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 152.4 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 152.4 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 152.4 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 152.4 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 152.4 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 152.4 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 152.4 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 152.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Dy3Fe5O12 (mp-645157) | 0.5629 | 0.022 | 3 |
Fe5(SiO4)3 (mp-566529) | 0.3556 | 0.289 | 3 |
Ho3Fe5O12 (mp-781609) | 0.5630 | 0.029 | 3 |
Gd3Fe5O12 (mp-585960) | 0.5306 | 1.542 | 3 |
Mn5(SiO4)3 (mp-19675) | 0.3381 | 0.079 | 3 |
Y2Co3(SiO4)3 (mvc-4297) | 0.0584 | 0.187 | 4 |
Mg3Si3(SnO6)2 (mvc-3630) | 0.0768 | 0.275 | 4 |
Mg3Si3(BiO6)2 (mvc-3636) | 0.0851 | 0.260 | 4 |
Zn3Si3(BiO6)2 (mvc-3675) | 0.0813 | 0.292 | 4 |
Zn3Si3(SbO6)2 (mvc-3660) | 0.0628 | 0.311 | 4 |
Ca3Ga2Si(SnO6)2 (mp-695070) | 0.4181 | 0.000 | 5 |
Na3Ca10Mn7V12O48 (mp-694988) | 0.4128 | 0.207 | 5 |
Li6MnV3(PO4)6 (mp-775157) | 0.3710 | 0.069 | 5 |
NaCa2Mg2(AsO4)3 (mp-677573) | 0.4070 | 0.000 | 5 |
Li3MnV(PO4)3 (mp-778558) | 0.4016 | 0.090 | 5 |
Ca11YAl15Cr4SiO48 (mp-743917) | 0.6339 | 0.116 | 6 |
Ca3Y9Al18CrSiO48 (mp-744910) | 0.6558 | 0.021 | 6 |
Ca4Y2Al7Cr2SiO24 (mp-743704) | 0.6578 | 0.104 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Si Sb O |
Final Energy/Atom-6.6115 eV |
Corrected Energy-561.9000 eV
Uncorrected energy = -528.9240 eV
Composition-based energy adjustment (-0.687 eV/atom x 48.0 atoms) = -32.9760 eV
Corrected energy = -561.9000 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)