Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.954 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.037 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.20 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa(NiO2)2 + CaO + O2 |
Band Gap0.007 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmc21 [36] |
HallC 2c 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 143.5 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 86.1 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 28.7 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 102.9 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 172.2 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 315.7 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 106.8 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 200.9 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 258.3 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 315.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 205.8 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 315.7 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 258.3 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 315.7 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 86.1 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 213.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 214.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 86.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 258.3 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 143.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 102.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 143.5 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 344.4 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 258.3 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 143.5 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 200.9 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 258.3 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 315.7 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 229.6 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 143.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 315.7 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 200.9 |
BN (mp-984) | <0 0 1> | <0 1 0> | 315.7 |
BN (mp-984) | <1 1 0> | <0 1 0> | 172.2 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 0> | 315.7 |
BN (mp-984) | <1 0 0> | <0 1 0> | 57.4 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 143.5 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 229.6 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 86.1 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 1> | 145.9 |
MoS2 (mp-1434) | <1 1 0> | <0 1 0> | 114.8 |
Al (mp-134) | <1 0 0> | <0 1 0> | 143.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 344.4 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 102.9 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 86.1 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 287.0 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 229.6 |
TeO2 (mp-2125) | <1 1 0> | <0 1 0> | 287.0 |
SiC (mp-7631) | <1 0 0> | <0 1 0> | 229.6 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 200.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca3Co2O7 (mvc-3670) | 0.1159 | 0.055 | 3 |
Ca3Mn2O7 (mp-19042) | 0.1406 | 0.016 | 3 |
Ca3Mn2O7 (mvc-11576) | 0.1253 | 0.016 | 3 |
Ca4Mn3O10 (mp-565885) | 0.1694 | 0.021 | 3 |
Ca4Mn3O10 (mp-622174) | 0.1674 | 0.021 | 3 |
LiLa3Ti2O9 (mp-766995) | 0.2830 | 0.030 | 4 |
NaSr4(SbO4)3 (mp-17433) | 0.2941 | 0.022 | 4 |
Sr3CaRu2O9 (mp-557111) | 0.3158 | 0.000 | 4 |
Sr2ErMoO6 (mp-18744) | 0.3486 | 0.000 | 4 |
CaPr(CoO3)2 (mvc-9638) | 0.3039 | 0.026 | 4 |
Pb3O4 (mp-636813) | 0.7017 | 0.037 | 2 |
Ca14La6Mg3Ti17O60 (mp-695227) | 0.2959 | 0.012 | 5 |
NaCa9TaTi9O30 (mp-677027) | 0.2792 | 0.002 | 5 |
Ca9LaTi8Mn2O30 (mp-694916) | 0.2973 | 0.009 | 5 |
Ca10Ti8NbFeO30 (mp-743819) | 0.2818 | 0.004 | 5 |
Na3Ca7Ta3Ti7O30 (mp-694044) | 0.2948 | 0.010 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Ca_sv Ni_pv O |
Final Energy/Atom-5.5312 eV |
Corrected Energy-151.2371 eV
-151.2371 eV = -132.7490 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction) - 8.6560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)