Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.578 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.093 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVF3 + CaF2 |
Band Gap0.249 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 246.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 172.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 229.7 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 241.6 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 113.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 241.0 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 172.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 229.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 229.7 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 287.6 |
BaF2 (mp-1029) | <1 1 1> | <1 1 0> | 270.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 287.1 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 205.4 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 246.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 57.4 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 211.8 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 282.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 57.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 287.1 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 287.1 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 287.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 229.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 229.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 282.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 229.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 241.0 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 287.6 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 270.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 229.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 229.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 211.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 114.8 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 123.2 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 205.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 287.6 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 287.1 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 205.4 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 287.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 241.0 |
GaSe (mp-1943) | <1 0 0> | <1 1 0> | 270.7 |
BN (mp-984) | <0 0 1> | <1 1 -1> | 273.1 |
BN (mp-984) | <1 0 0> | <0 1 1> | 211.8 |
BN (mp-984) | <1 0 1> | <0 1 0> | 328.6 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 287.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 123.2 |
Al (mp-134) | <1 0 0> | <0 1 1> | 211.8 |
Al (mp-134) | <1 1 0> | <0 0 1> | 114.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 57.4 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 287.1 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 1> | 141.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaTiF5 (mvc-3419) | 0.1046 | 0.026 | 3 |
CaFeF5 (mvc-11613) | 0.0680 | 0.121 | 3 |
CaCrF5 (mvc-3731) | 0.1193 | 0.141 | 3 |
CaFeF5 (mp-630865) | 0.0735 | 0.121 | 3 |
CaCuF5 (mvc-3399) | 0.1118 | 0.024 | 3 |
U2O5 (mp-647814) | 0.6947 | 0.017 | 2 |
U3O8 (mp-559906) | 0.6914 | 0.003 | 2 |
Np2O5 (mp-554714) | 0.5430 | 0.000 | 2 |
U3O8 (mp-560402) | 0.6506 | 0.012 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Ca_sv V_pv F |
Final Energy/Atom-5.9355 eV |
Corrected Energy-182.2336 eV
Uncorrected energy = -166.1936 eV
Composition-based energy adjustment (-0.462 eV/atom x 20.0 atoms) = -9.2400 eV
Composition-based energy adjustment (-1.700 eV/atom x 4.0 atoms) = -6.8000 eV
Corrected energy = -182.2336 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)