Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.777 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.134 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZn(SbO3)2 + SnO2 + Sb2O3 + ZnO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 206.1 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 175.4 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 248.2 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 29.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 131.5 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 88.3 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 248.2 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 248.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 219.2 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 235.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 158.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 43.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 52.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 186.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 131.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 0> | 211.3 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 147.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 131.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 186.2 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 147.2 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 306.9 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 235.5 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 219.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 131.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 186.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 350.8 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 310.3 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 294.4 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 124.1 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 265.0 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 186.2 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 87.7 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 211.3 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 263.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 131.5 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 186.2 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 274.8 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 263.1 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 316.9 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 211.3 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 323.9 |
YVO4 (mp-19133) | <1 1 1> | <1 0 1> | 248.2 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 316.9 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 235.5 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 274.8 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 175.4 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 235.5 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 147.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 88.3 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 206.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnSnO3 (mvc-13441) | 0.1231 | 0.083 | 3 |
MgWO3 (mvc-5026) | 0.1922 | 0.088 | 3 |
ZnMoO3 (mvc-4002) | 0.1673 | 0.086 | 3 |
Li3MnF6 (mp-764288) | 0.1988 | 0.029 | 3 |
LiFeF3 (mp-776189) | 0.1204 | 0.039 | 3 |
Zn2SnIrO6 (mvc-5623) | 0.1783 | 0.151 | 4 |
Zn2CrWO6 (mvc-5100) | 0.2317 | 0.091 | 4 |
VZn2WO6 (mvc-5045) | 0.1927 | 0.081 | 4 |
Zn2SbMoO6 (mvc-13704) | 0.1576 | 0.143 | 4 |
Zn2CrIrO6 (mvc-5807) | 0.2062 | 0.117 | 4 |
V3O5 (mp-714914) | 0.5284 | 0.004 | 2 |
V3O5 (mp-714911) | 0.5382 | 0.003 | 2 |
V3O5 (mp-622497) | 0.5544 | 0.004 | 2 |
V3O5 (mp-542441) | 0.5304 | 0.029 | 2 |
Ti4O7 (mp-12205) | 0.5811 | 0.005 | 2 |
Li4CrSb(WO6)2 (mp-764950) | 0.5291 | 0.037 | 5 |
Li4CrTe2WO12 (mp-775509) | 0.5203 | 0.109 | 5 |
Li4FeTe2WO12 (mp-775176) | 0.5255 | 0.073 | 5 |
Li4MnSb2WO12 (mp-763536) | 0.5303 | 0.069 | 5 |
Li4CrSb(TeO6)2 (mp-781050) | 0.5213 | 0.048 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zn Sn_d Sb O |
Final Energy/Atom-5.3901 eV |
Corrected Energy-116.2296 eV
-116.2296 eV = -107.8022 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)