Final Magnetic Moment1.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.038 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.065 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.54 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa2Co3O8 + CaO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 49.0 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 143.4 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 119.1 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 1> | 244.9 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 146.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 86.1 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 198.5 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 79.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 86.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 172.1 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 195.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 121.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 258.2 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 158.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 86.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 28.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 143.4 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 277.9 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 121.6 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 81.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 258.2 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 158.8 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 283.7 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 143.4 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 119.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 158.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 258.2 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 244.9 |
KCl (mp-23193) | <1 1 1> | <0 1 1> | 146.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 119.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 86.1 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 317.6 |
ZnSe (mp-1190) | <1 1 1> | <0 1 1> | 342.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 317.9 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 158.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 258.2 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 277.9 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 248.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 258.2 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 283.7 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 198.5 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 202.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 258.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 195.9 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 248.3 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 119.1 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 317.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 258.2 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 200.8 |
TePb (mp-19717) | <1 1 1> | <0 1 1> | 146.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaNiO3 (mvc-3998) | 0.1137 | 0.053 | 3 |
CaCrO3 (mp-24909) | 0.1046 | 0.056 | 3 |
CaCrO3 (mvc-11968) | 0.0602 | 0.056 | 3 |
YbFeO3 (mp-24951) | 0.1244 | 0.000 | 3 |
CaVO3 (mp-25150) | 0.1263 | 0.001 | 3 |
Sr2UZnO6 (mp-554059) | 0.1897 | 0.054 | 4 |
CaPrTi2O6 (mvc-9241) | 0.2108 | 0.000 | 4 |
CaPrCr2O6 (mvc-9616) | 0.1834 | 0.042 | 4 |
CaPrV2O6 (mvc-9618) | 0.1725 | 0.015 | 4 |
CaPr(FeO3)2 (mvc-9650) | 0.1747 | 0.000 | 4 |
SrLaNiRuO6 (mp-694873) | 0.2096 | 0.000 | 5 |
Ca5Yb3Ti5Mn3O24 (mp-698722) | 0.1492 | 0.008 | 5 |
CaLaCrCuO6 (mvc-10031) | 0.1903 | 0.129 | 5 |
CaLaTiMnO6 (mvc-16554) | 0.2297 | 0.086 | 5 |
CaLaCrCoO6 (mvc-9966) | 0.2206 | 0.119 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Ca_sv Co O |
Final Energy/Atom-6.0331 eV |
Corrected Energy-136.5850 eV
-136.5850 eV = -120.6615 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 7.4960 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)