Final Magnetic Moment1.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.515 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.144 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMg(CuO2)2 + MgTa2O6 + Mg4Ta2O9 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 204.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 224.1 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 81.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 286.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 40.9 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 204.4 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 196.1 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 196.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 116.4 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 196.1 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 155.2 |
KCl (mp-23193) | <1 0 0> | <1 1 1> | 322.2 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 224.1 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 196.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 194.0 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 140.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 58.0 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 322.2 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 163.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 116.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 122.6 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 81.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 168.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 286.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 122.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 163.5 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 163.5 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 327.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 310.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 140.1 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 168.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 310.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 155.2 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 252.1 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 271.6 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 271.6 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 218.5 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 140.1 |
BN (mp-984) | <0 0 1> | <0 1 1> | 143.6 |
BN (mp-984) | <1 1 0> | <1 0 0> | 163.5 |
BN (mp-984) | <1 1 1> | <1 0 1> | 232.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 196.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 155.2 |
Te2W (mp-22693) | <1 1 0> | <1 0 -1> | 109.2 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 0> | 224.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 168.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 155.2 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 273.1 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 273.1 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 198.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnZnO3 (mvc-3995) | 0.2237 | 0.098 | 3 |
MgTiO3 (mvc-3783) | 0.2466 | 0.083 | 3 |
MgVO3 (mvc-15888) | 0.2480 | 0.093 | 3 |
ZnCoO3 (mvc-15868) | 0.2465 | 0.157 | 3 |
GdLuO3 (mp-756424) | 0.2416 | 0.056 | 3 |
Mg2TaNiO6 (mvc-4367) | 0.1639 | 0.124 | 4 |
Mg2TaMnO6 (mvc-4366) | 0.1751 | 0.098 | 4 |
Mg2TaVO6 (mvc-4360) | 0.1597 | 0.134 | 4 |
Mg2TaFeO6 (mvc-4359) | 0.1536 | 0.258 | 4 |
Mg2TaCrO6 (mvc-4358) | 0.1724 | 0.721 | 4 |
Al2O3 (mp-642363) | 0.6594 | 0.280 | 2 |
Te2Ir (mp-569388) | 0.6402 | 0.000 | 2 |
V3O5 (mp-542441) | 0.6297 | 0.029 | 2 |
Ti3O5 (mp-556754) | 0.6485 | 0.013 | 2 |
Ti4O7 (mp-558097) | 0.6618 | 0.005 | 2 |
LiCa3Zr3TaO12 (mp-677136) | 0.4410 | 0.004 | 5 |
Mg3AlFe(SiO4)3 (mp-699146) | 0.4405 | 0.311 | 5 |
LaMgCrMoO6 (mvc-9867) | 0.4509 | 0.712 | 5 |
LaMgCrSbO6 (mvc-9859) | 0.4530 | 0.842 | 5 |
LaMgCrSnO6 (mvc-9925) | 0.4620 | 0.773 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Ta_pv Cu_pv O |
Final Energy/Atom-6.9778 eV |
Corrected Energy-147.9828 eV
-147.9828 eV = -139.5553 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)