Final Magnetic Moment12.012 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.918 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.198 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToY2Si2O7 + SiO2 + Cr2O3 + Cr |
Band Gap2.177 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIa3d [230] |
Hall-I 4bd 2c 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 155.0 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 155.0 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 155.0 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 155.0 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 155.0 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 155.0 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 155.0 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 155.0 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 155.0 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 155.0 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 155.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe5(SiO4)3 (mp-566529) | 0.3277 | 0.289 | 3 |
Gd3Fe5O12 (mp-585960) | 0.4991 | 1.542 | 3 |
Mn5(SiO4)3 (mp-19675) | 0.3047 | 0.079 | 3 |
Ho3Ga5O12 (mp-15575) | 0.5411 | 0.000 | 3 |
Y3Fe5O12 (mp-565957) | 0.5407 | 0.024 | 3 |
Y2V3(SiO4)3 (mvc-4290) | 0.0897 | 0.194 | 4 |
Y2Cu3(SiO4)3 (mvc-4085) | 0.0213 | 0.317 | 4 |
Y2Si3(NiO4)3 (mvc-4333) | 0.0948 | 0.267 | 4 |
Ca3Ge3(BiO6)2 (mvc-4268) | 0.1235 | 0.048 | 4 |
Zn3Si3(SbO6)2 (mvc-3660) | 0.1412 | 0.311 | 4 |
Na3Ca10Mn7V12O48 (mp-694988) | 0.4096 | 0.207 | 5 |
Li3MnV(PO4)3 (mp-779826) | 0.4018 | 0.142 | 5 |
Li6MnV3(PO4)6 (mp-775157) | 0.3568 | 0.069 | 5 |
NaCa2Mg2(AsO4)3 (mp-677573) | 0.4052 | 0.000 | 5 |
Li3MnV(PO4)3 (mp-778558) | 0.3560 | 0.090 | 5 |
Ca11YAl15Cr4SiO48 (mp-743917) | 0.5930 | 0.116 | 6 |
Ca3Y9Al18CrSiO48 (mp-744910) | 0.6178 | 0.021 | 6 |
Ca4Y2Al7Cr2SiO24 (mp-743704) | 0.6094 | 0.104 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Y_sv Cr_pv Si O |
Final Energy/Atom-8.0717 eV |
Corrected Energy-702.7019 eV
Uncorrected energy = -645.7379 eV
Composition-based energy adjustment (-0.687 eV/atom x 48.0 atoms) = -32.9760 eV
Composition-based energy adjustment (-1.999 eV/atom x 12.0 atoms) = -23.9880 eV
Corrected energy = -702.7019 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)