Final Magnetic Moment0.991 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.240 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.138 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.31 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTa2Zn3O8 + ZnO + Mo + MoO2 |
Band Gap1.446 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 211.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 154.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 211.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 60.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 42.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 211.8 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 304.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 169.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 84.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 211.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 338.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 211.8 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 320.2 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 257.0 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 169.5 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 202.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 127.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 42.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 182.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 320.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 60.8 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 205.6 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 349.3 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 304.2 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 232.9 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 232.9 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 205.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 127.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 304.2 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 304.2 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 254.2 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 320.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 296.6 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 169.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 254.2 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 320.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 296.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 211.8 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 304.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 304.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 87.3 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 202.4 |
GaSe (mp-1943) | <1 0 0> | <0 1 0> | 262.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 182.5 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 297.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 169.5 |
BN (mp-984) | <1 0 0> | <0 1 0> | 58.2 |
BN (mp-984) | <1 1 1> | <1 0 0> | 169.8 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 304.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 203.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3VF6 (mp-764965) | 0.2501 | 0.069 | 3 |
Li3MnF6 (mp-764288) | 0.2163 | 0.182 | 3 |
ZnSbO3 (mvc-3953) | 0.2370 | 0.161 | 3 |
HfCoO3 (mp-765829) | 0.2380 | 0.095 | 3 |
CoSnO3 (mp-765815) | 0.2329 | 0.269 | 3 |
Zn2MoWO6 (mvc-5052) | 0.1991 | 0.037 | 4 |
Zn2CoWO6 (mvc-5043) | 0.2045 | 0.085 | 4 |
Zn2NiWO6 (mvc-5021) | 0.1979 | 0.084 | 4 |
TaZn2WO6 (mvc-4407) | 0.0811 | 0.208 | 4 |
Zn2NiIrO6 (mvc-5861) | 0.1872 | 0.017 | 4 |
V3O5 (mp-714914) | 0.5369 | 0.004 | 2 |
Te2Ir (mp-569388) | 0.5085 | 0.000 | 2 |
V3O5 (mp-542441) | 0.5021 | 0.029 | 2 |
Ti4O7 (mp-12205) | 0.5423 | 0.007 | 2 |
Ti4O7 (mp-558097) | 0.5412 | 0.007 | 2 |
Li4MnSn(WO6)2 (mp-775961) | 0.4165 | 0.050 | 5 |
Li4FeSb(TeO6)2 (mp-780741) | 0.4369 | 3.378 | 5 |
Li4CrTe2WO12 (mp-775509) | 0.4430 | 0.109 | 5 |
Li4CrSb(TeO6)2 (mp-781050) | 0.4190 | 0.048 | 5 |
Li4FeSb(WO6)2 (mp-767012) | 0.4414 | 3.405 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMo: 4.38 eV |
PseudopotentialsVASP PAW: Ta_pv Zn Mo_pv O |
Final Energy/Atom-6.9569 eV |
Corrected Energy-153.7855 eV
Uncorrected energy = -139.1375 eV
Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV
Composition-based energy adjustment (-3.202 eV/atom x 2.0 atoms) = -6.4040 eV
Corrected energy = -153.7855 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)