Final Magnetic Moment3.680 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.947 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.204 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.49 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAg3O4 + MgO + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 163.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 81.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 115.3 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 81.5 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 115.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 163.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 81.5 |
MoS2 (mp-1434) | <0 0 1> | <1 1 1> | 141.2 |
Al (mp-134) | <1 0 0> | <1 0 0> | 81.5 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 163.0 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 230.6 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 244.6 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 230.6 |
Mg (mp-153) | <0 0 1> | <1 1 1> | 141.2 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 163.0 |
WS2 (mp-224) | <0 0 1> | <1 1 1> | 141.2 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 81.5 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 163.0 |
Ga2O3 (mp-886) | <1 0 -1> | <1 1 0> | 115.3 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 230.6 |
MgF2 (mp-1249) | <1 1 1> | <1 0 0> | 244.6 |
GaTe (mp-542812) | <0 0 1> | <1 1 0> | 230.6 |
GaTe (mp-542812) | <1 0 -1> | <1 1 0> | 230.6 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 163.0 |
Al2O3 (mp-1143) | <0 0 1> | <1 1 1> | 141.2 |
YAlO3 (mp-3792) | <0 1 0> | <1 1 0> | 115.3 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 0> | 244.6 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 163.0 |
SiC (mp-8062) | <1 0 0> | <1 1 0> | 115.3 |
Fe2O3 (mp-24972) | <1 1 0> | <1 0 0> | 244.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn(AgO2)2 (mvc-4660) | 0.0124 | 0.171 | 3 |
Sc2FeS4 (mp-20499) | 0.0249 | 0.113 | 3 |
Mg2FeO4 (mp-771287) | 0.0247 | 0.096 | 3 |
Mg(SnO2)2 (mvc-4659) | 0.0220 | 0.344 | 3 |
Lu2MnS4 (mp-14305) | 0.0254 | 0.000 | 3 |
Cr4FeCuS8 (mp-6685) | 0.1874 | 0.037 | 4 |
Li2V3CrO8 (mp-853131) | 0.2619 | 0.033 | 4 |
LiZn(Fe5O8)2 (mp-773267) | 0.2445 | 0.081 | 4 |
Li2VFe3O8 (mp-771748) | 0.2472 | 0.079 | 4 |
LiCr3(FeO4)2 (mp-771630) | 0.2610 | 0.439 | 4 |
Co3S4 (mp-943) | 0.1160 | 0.000 | 2 |
Fe3S4 (mp-21515) | 0.0453 | 0.136 | 2 |
Cr3N4 (mp-1014379) | 0.0233 | 0.105 | 2 |
C3N4 (mp-563) | 0.0700 | 1.498 | 2 |
Si3N4 (mp-2075) | 0.1280 | 0.147 | 2 |
Li4Ti3Cr3(WO8)2 (mp-773537) | 0.3957 | 0.043 | 5 |
Li4Fe3Ni3(TeO8)2 (mp-773382) | 0.3851 | 0.009 | 5 |
Li4Mn3Cr3(CuO8)2 (mp-765456) | 0.3862 | 0.080 | 5 |
Li4Cr3Cu3(SbO8)2 (mp-783908) | 0.3980 | 0.040 | 5 |
Li4Cr3Fe3(SbO8)2 (mp-771925) | 0.3785 | 0.831 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.7049 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6968 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.7014 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.7041 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6950 | 0.032 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Ag O |
Final Energy/Atom-4.4106 eV |
Corrected Energy-67.3672 eV
-67.3672 eV = -61.7489 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)