Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.088 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.062 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa(BiO2)2 |
Band Gap1.861 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <0 0 1> | <0 0 1> | 170.9 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 256.4 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 170.9 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 256.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 256.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 170.9 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 256.4 |
C (mp-66) | <1 0 0> | <0 0 1> | 256.4 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 256.4 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 256.4 |
Ni (mp-23) | <1 0 0> | <1 0 1> | 197.5 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 256.4 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 256.4 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 170.9 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 256.4 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 256.4 |
Ge (mp-32) | <1 1 1> | <0 0 1> | 170.9 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 256.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca(BiO2)2 (mvc-5187) | 0.0699 | 0.058 | 3 |
MgV2O4 (mvc-5074) | 0.0699 | 0.052 | 3 |
Mg(FeO2)2 (mp-34569) | 0.0610 | 0.036 | 3 |
Ho2CdS4 (mp-531811) | 0.0656 | 0.062 | 3 |
Mg(FeO2)2 (mp-33325) | 0.0594 | 0.035 | 3 |
LiZn2Fe9O16 (mp-773576) | 0.1126 | 0.065 | 4 |
LiZn4Fe13O24 (mp-769606) | 0.1315 | 0.075 | 4 |
LiZn2Fe9O16 (mp-771993) | 0.1260 | 0.057 | 4 |
LiZnFe7O12 (mp-771267) | 0.1004 | 0.054 | 4 |
Li3Zn2Fe19O32 (mp-771170) | 0.1018 | 0.065 | 4 |
Fe3O4 (mp-715491) | 0.1806 | 0.020 | 2 |
Fe3O4 (mp-542433) | 0.1777 | 0.034 | 2 |
Fe3O4 (mp-31770) | 0.1866 | 0.020 | 2 |
Fe3O4 (mp-715558) | 0.1725 | 0.018 | 2 |
Fe3O4 (mp-715811) | 0.1787 | 0.018 | 2 |
Li4Ti3Cr3(SnO8)2 (mp-776780) | 0.2334 | 0.027 | 5 |
Li14Mn22Cr3Cu3O56 (mp-735790) | 0.2405 | 0.021 | 5 |
Li4Ti3Cr3(WO8)2 (mp-773537) | 0.2359 | 0.042 | 5 |
Li4Cr3Fe3(TeO8)2 (mp-773518) | 0.2304 | 0.024 | 5 |
Li4Cr3Fe3(SbO8)2 (mp-771925) | 0.2608 | 0.060 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.7387 | 0.030 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.7430 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.7497 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.7442 | 0.062 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.7479 | 0.012 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Bi O |
Final Energy/Atom-5.9093 eV |
Corrected Energy-353.3930 eV
-353.3930 eV = -330.9197 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)