Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.296 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.077 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.55 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNb2NiO6 + ZnO |
Band Gap2.811 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdS (mp-672) | <1 0 0> | <1 0 0> | 249.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 342.7 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 118.1 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 118.1 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 201.3 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 280.4 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 201.3 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 249.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 342.7 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 280.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 280.4 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 124.6 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 118.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 124.6 |
BN (mp-984) | <0 0 1> | <1 0 0> | 218.1 |
BN (mp-984) | <1 0 0> | <1 0 0> | 280.4 |
BN (mp-984) | <1 0 1> | <1 0 0> | 280.4 |
BN (mp-984) | <1 1 0> | <1 0 0> | 280.4 |
BN (mp-984) | <1 1 1> | <1 0 0> | 280.4 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 93.5 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 218.1 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 0> | 155.8 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 280.4 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 280.4 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 342.7 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 124.6 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 201.3 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 155.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 227.3 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 342.7 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 280.4 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 280.4 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 100.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 249.2 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 201.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 249.2 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 280.4 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 280.4 |
SiC (mp-7631) | <1 1 0> | <1 0 0> | 155.8 |
SiC (mp-7631) | <1 1 1> | <1 0 0> | 155.8 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 93.5 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 218.1 |
LiTaO3 (mp-3666) | <1 0 1> | <1 0 0> | 155.8 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 280.4 |
Fe3O4 (mp-19306) | <1 1 1> | <1 0 0> | 124.6 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 218.1 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 124.6 |
TiO2 (mp-2657) | <1 1 0> | <1 0 1> | 118.1 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 249.2 |
C (mp-66) | <1 0 0> | <1 0 0> | 155.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3CuF6 (mp-759234) | 0.4094 | 0.027 | 3 |
Li3VF6 (mp-763439) | 0.3944 | 0.037 | 3 |
Nb2Zn3O8 (mp-18575) | 0.1218 | 0.023 | 3 |
Li3FeF6 (mp-776684) | 0.4043 | 0.170 | 3 |
Li3AlF6 (mp-556020) | 0.4129 | 0.006 | 3 |
MnNb2Zn2O8 (mvc-15008) | 0.1780 | 0.191 | 4 |
Ta2Zn2NiO8 (mvc-2670) | 0.1690 | 0.008 | 4 |
Nb2Zn2FeO8 (mvc-3393) | 0.1057 | 0.198 | 4 |
Nb2Zn2CoO8 (mvc-417) | 0.0425 | 0.078 | 4 |
Nb2VZn2O8 (mvc-423) | 0.1179 | 0.019 | 4 |
V5O9 (mp-714932) | 0.3413 | 0.017 | 2 |
V5O9 (mp-558587) | 0.4022 | 0.008 | 2 |
V7O13 (mp-715598) | 0.4093 | 0.143 | 2 |
Ti4O7 (mp-558097) | 0.4201 | 0.007 | 2 |
V5O9 (mp-704305) | 0.3501 | 0.008 | 2 |
Li4FeTe(WO6)2 (mp-771716) | 0.3671 | 0.163 | 5 |
Li4MnNb2WO12 (mp-771475) | 0.3797 | 0.044 | 5 |
Li4CrTe2WO12 (mp-775509) | 0.4102 | 0.109 | 5 |
Li4MnSb(WO6)2 (mp-779994) | 0.3933 | 0.041 | 5 |
Li4FeTe2WO12 (mp-775176) | 0.3746 | 0.208 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Nb_pv Zn Ni_pv O |
Final Energy/Atom-6.9344 eV |
Corrected Energy-196.3693 eV
Uncorrected energy = -180.2953 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Composition-based energy adjustment (-2.541 eV/atom x 2.0 atoms) = -5.0820 eV
Corrected energy = -196.3693 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)