Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.579 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.097 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.75 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBiO2 + SiO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 52.3 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 261.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 196.0 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 94.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 125.5 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 316.4 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 156.9 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 125.5 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 297.1 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 261.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 209.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 209.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 261.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 52.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 313.7 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 209.2 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 316.4 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 251.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 283.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 156.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 283.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 313.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 158.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 283.4 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 104.6 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 158.2 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 209.2 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 261.4 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 313.7 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 283.4 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 211.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 196.0 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 196.0 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 125.5 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 156.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 -1> | 188.9 |
BN (mp-984) | <1 0 0> | <1 1 -1> | 216.4 |
BN (mp-984) | <1 0 1> | <1 1 0> | 297.1 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 313.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 294.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 104.6 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 52.3 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 209.2 |
BN (mp-984) | <0 0 1> | <1 0 0> | 104.6 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 294.1 |
Al (mp-134) | <1 1 0> | <0 1 0> | 158.2 |
Al (mp-134) | <1 1 1> | <1 0 -1> | 283.4 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 0> | 297.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 263.7 |
LiGaO2 (mp-5854) | <1 1 1> | <1 1 0> | 222.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn(PO3)2 (mp-8230) | 0.3194 | 0.013 | 3 |
Si2SnO6 (mvc-4955) | 0.3650 | 0.065 | 3 |
Si2SbO6 (mvc-4921) | 0.2433 | 0.154 | 3 |
CoPO4 (mp-510669) | 0.3690 | 0.197 | 3 |
Cu(PO3)2 (mp-25976) | 0.3336 | 0.012 | 3 |
MnFe3(PO4)4 (mp-767822) | 0.4989 | 0.449 | 4 |
VFe(PO4)2 (mp-775394) | 0.4878 | 0.200 | 4 |
FeSb(PO4)2 (mp-861596) | 0.4950 | 0.062 | 4 |
Mn3Co(PO4)4 (mp-761652) | 0.4837 | 0.184 | 4 |
LiTi(PO3)4 (mp-757996) | 0.4805 | 0.073 | 4 |
MnFeCo(PO4)3 (mp-764392) | 0.5381 | 0.028 | 5 |
MnFeCo(PO4)3 (mp-763496) | 0.5362 | 0.026 | 5 |
MnFeCo(PO4)3 (mp-764415) | 0.5663 | 0.035 | 5 |
MnFeCo(PO4)3 (mp-764383) | 0.5187 | 0.038 | 5 |
MnFeCo(PO4)3 (mp-764739) | 0.5252 | 0.023 | 5 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.7379 | 0.001 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si Bi O |
Final Energy/Atom-7.0460 eV |
Corrected Energy-135.0726 eV
Uncorrected energy = -126.8286 eV
Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV
Corrected energy = -135.0726 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)