Final Magnetic Moment4.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.672 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.027 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZn2SiO4 + Fe2SiO4 + SiO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 50.0 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 250.1 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 250.1 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 237.9 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 247.3 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 281.4 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 346.2 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 150.1 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 346.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 247.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 300.1 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 197.8 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 150.1 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 247.3 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 150.1 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 200.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 277.2 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 247.3 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 300.1 |
LiGaO2 (mp-5854) | <1 1 1> | <1 1 0> | 211.0 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 184.8 |
CdTe (mp-406) | <1 1 1> | <1 0 0> | 150.1 |
SiC (mp-7631) | <1 0 1> | <1 0 1> | 237.9 |
SiC (mp-7631) | <1 1 0> | <0 1 0> | 247.3 |
MgO (mp-1265) | <1 1 1> | <0 1 0> | 346.2 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 197.8 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 247.3 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 250.1 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 197.8 |
C (mp-66) | <1 1 0> | <0 1 0> | 197.8 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 0> | 296.8 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 277.2 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 -1> | 267.1 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 346.2 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 50.0 |
Mg (mp-153) | <1 0 1> | <0 1 1> | 209.6 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 150.1 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 200.1 |
PbS (mp-21276) | <1 0 0> | <1 0 -1> | 178.0 |
GaP (mp-2490) | <1 1 0> | <1 0 0> | 250.1 |
InP (mp-20351) | <1 0 0> | <1 0 -1> | 178.0 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 150.1 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 250.1 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 277.2 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 -1> | 267.1 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 250.1 |
InSb (mp-20012) | <1 0 0> | <1 0 -1> | 89.0 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 184.8 |
InSb (mp-20012) | <1 1 1> | <1 0 0> | 150.1 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 296.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnSiO3 (mp-619034) | 0.4190 | 0.054 | 3 |
ZnSiO3 (mp-562182) | 0.3980 | 0.049 | 3 |
FeSiO3 (mp-510602) | 0.2199 | 0.017 | 3 |
MgSiO3 (mp-1020115) | 0.4305 | 0.031 | 3 |
FeSiO3 (mp-562679) | 0.2939 | 0.017 | 3 |
ZnSi2NiO6 (mvc-5138) | 0.1231 | 0.028 | 4 |
ZnCo(SiO3)2 (mvc-5137) | 0.1050 | 0.028 | 4 |
MgFe(SiO3)2 (mvc-5134) | 0.1939 | 0.029 | 4 |
VZn(SiO3)2 (mvc-5127) | 0.1169 | 0.042 | 4 |
MgMn(SiO3)2 (mvc-5116) | 0.1254 | 0.026 | 4 |
Li7Sc9Fe(SiO3)20 (mp-764979) | 0.4646 | 0.040 | 5 |
Li8Sc5Fe3(SiO3)16 (mp-775186) | 0.5190 | 0.004 | 5 |
Li5Sc2Fe3(SiO3)10 (mp-775172) | 0.5767 | 0.005 | 5 |
Li7Sc9Fe(SiO3)20 (mp-851054) | 0.5070 | 0.060 | 5 |
Li2MnV4FeO12 (mp-776234) | 0.5878 | 0.064 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Zn Fe_pv Si O |
Final Energy/Atom-7.0041 eV |
Corrected Energy-153.9749 eV
-153.9749 eV = -140.0814 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)