Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.694 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.074 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZnCr2O4 + SiO2 + Zn |
Band Gap0.102 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 150.2 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 51.1 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 204.3 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 150.2 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 51.1 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 123.9 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 255.4 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 143.0 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 200.2 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 214.5 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 204.3 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 300.3 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 204.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 51.1 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 150.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 150.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 51.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 273.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 287.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 306.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 214.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 204.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 287.9 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 200.2 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 191.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 287.9 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 153.2 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 100.1 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 286.1 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 200.2 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 123.9 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 286.1 |
BN (mp-984) | <1 0 0> | <1 0 0> | 153.2 |
BN (mp-984) | <0 0 1> | <0 1 0> | 250.3 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 150.2 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 204.3 |
MoS2 (mp-1434) | <1 0 1> | <1 1 -1> | 207.8 |
Al (mp-134) | <1 0 0> | <1 0 0> | 306.5 |
Al (mp-134) | <1 1 1> | <0 0 1> | 287.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 300.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 0> | 286.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 300.3 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 102.2 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 0> | 214.5 |
LiGaO2 (mp-5854) | <1 1 1> | <1 1 0> | 214.5 |
CdTe (mp-406) | <1 0 0> | <1 0 -1> | 91.1 |
CdTe (mp-406) | <1 1 1> | <1 0 0> | 153.2 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 123.9 |
SiC (mp-7631) | <0 0 1> | <1 1 0> | 214.5 |
SiC (mp-7631) | <1 1 1> | <0 1 0> | 250.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnSiO3 (mp-619034) | 0.4811 | 0.054 | 3 |
ZnSiO3 (mp-562182) | 0.2819 | 0.049 | 3 |
FeSiO3 (mp-510602) | 0.3811 | 0.017 | 3 |
FeSiO3 (mp-562679) | 0.4360 | 0.017 | 3 |
MnSiO3 (mp-25041) | 0.5660 | 0.016 | 3 |
MnZn(SiO3)2 (mvc-5128) | 0.1176 | 0.021 | 4 |
MgCr(SiO3)2 (mvc-5119) | 0.1083 | 0.632 | 4 |
MgMn(SiO3)2 (mvc-5116) | 0.2030 | 0.026 | 4 |
MgCu(SiO3)2 (mvc-4926) | 0.2452 | 0.106 | 4 |
CaMg(SiO3)2 (mp-562517) | 0.2370 | 0.058 | 4 |
Li7Sc9Fe(SiO3)20 (mp-764979) | 0.5808 | 0.040 | 5 |
Li8Sc5Fe3(SiO3)16 (mp-775186) | 0.5972 | 0.004 | 5 |
Li5Sc2Fe3(SiO3)10 (mp-775172) | 0.6531 | 0.005 | 5 |
Li2ScFe(SiO3)4 (mp-772338) | 0.6695 | 0.007 | 5 |
Li7Sc9Fe(SiO3)20 (mp-851054) | 0.6073 | 0.060 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Zn Cr_pv Si O |
Final Energy/Atom-7.2165 eV |
Corrected Energy-156.7832 eV
-156.7832 eV = -144.3297 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 4.0260 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)