Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.680 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.163 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.16 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMoAs2O7 + MoO3 |
Band Gap1.787 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 301.9 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 1> | 283.9 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 218.6 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 312.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 60.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 255.2 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 301.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 301.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 301.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 204.1 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 218.6 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 204.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 208.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 218.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 181.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 60.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 204.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 301.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 260.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 204.1 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 312.2 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 204.1 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 239.1 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 158.1 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 301.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 255.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 306.2 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 218.6 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 306.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 301.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 204.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 204.1 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 237.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 153.1 |
BN (mp-984) | <1 0 0> | <1 0 1> | 79.1 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 94.6 |
BN (mp-984) | <1 1 0> | <0 0 1> | 102.1 |
BN (mp-984) | <1 1 1> | <0 1 0> | 104.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 204.1 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 153.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 318.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 301.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 181.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 204.1 |
Al (mp-134) | <1 1 0> | <1 0 0> | 181.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 204.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 301.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 102.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 51.0 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 255.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3N2O9 (mp-674942) | 0.6596 | 0.611 | 3 |
CrAsO5 (mvc-5643) | 0.4479 | 0.181 | 3 |
BiTeO5 (mvc-7469) | 0.6530 | 0.332 | 3 |
LiNi(PO3)3 (mp-861591) | 0.7434 | 0.091 | 4 |
VAs2H4O9 (mp-735567) | 0.7495 | 0.011 | 4 |
KSb(MoO4)2 (mp-618807) | 0.6619 | 0.020 | 4 |
V3H4NO8 (mp-768097) | 0.7476 | 0.103 | 4 |
VAs2H4O9 (mp-541267) | 0.7331 | 0.002 | 4 |
Se2O5 (mp-27358) | 0.7404 | 0.000 | 2 |
Li2FeP2HO8 (mp-705456) | 0.7180 | 0.180 | 5 |
Na4P2H4CO9 (mp-696155) | 0.6747 | 0.135 | 5 |
MnP3H10C3NO9 (mp-743546) | 0.7224 | 0.113 | 6 |
NaPH3C2N3O4 (mp-696990) | 0.7155 | 0.413 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMo: 4.38 eV |
PseudopotentialsVASP PAW: Mo_pv As O |
Final Energy/Atom-6.4230 eV |
Corrected Energy-208.0138 eV
-208.0138 eV = -179.8440 eV (uncorrected energy) - 14.1240 eV (MP Advanced Correction) - 14.0458 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)