Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.556 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.026 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.38 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNi2P2O7 + Mg2P2O7 |
Band Gap3.813 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 -1 1> | 127.8 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 213.5 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 314.6 |
LaAlO3 (mp-2920) | <1 1 1> | <1 -1 1> | 127.8 |
AlN (mp-661) | <0 0 1> | <1 -1 1> | 127.8 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 167.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 269.2 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 314.6 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 224.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 292.8 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 269.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 -1> | 231.4 |
GaAs (mp-2534) | <1 1 1> | <1 1 -1> | 231.4 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 267.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 278.4 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 53.4 |
GaN (mp-804) | <1 0 0> | <1 -1 1> | 255.5 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 267.2 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 292.8 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 269.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 318.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 314.6 |
SiO2 (mp-6930) | <1 0 1> | <1 1 -1> | 308.5 |
SiO2 (mp-6930) | <1 1 0> | <1 -1 -1> | 238.0 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 314.6 |
KCl (mp-23193) | <1 0 0> | <0 1 -1> | 285.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 278.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 346.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 -1> | 171.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 159.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 230.7 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 -1> | 285.7 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 267.2 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 269.2 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 269.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 -1> | 231.4 |
ZnSe (mp-1190) | <1 1 1> | <1 1 -1> | 231.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 161.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 161.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 314.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 119.3 |
CdS (mp-672) | <1 0 0> | <1 1 -1> | 231.4 |
CdS (mp-672) | <1 0 1> | <1 1 -1> | 231.4 |
CdS (mp-672) | <1 1 0> | <0 1 -1> | 285.7 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 314.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 198.9 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 161.9 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 314.6 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 238.7 |
Te2W (mp-22693) | <0 1 0> | <1 -1 1> | 319.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
VAsO4 (mp-761296) | 0.4945 | 0.060 | 3 |
NaPO3 (mp-558192) | 0.4454 | 0.006 | 3 |
V2P2O7 (mp-776066) | 0.4071 | 0.130 | 3 |
Hg2P2O7 (mp-28455) | 0.4437 | 0.000 | 3 |
Mn2P3O10 (mp-31981) | 0.4698 | 0.030 | 3 |
MgFeP2O7 (mvc-5721) | 0.1611 | 0.022 | 4 |
ZnFeP2O7 (mvc-5718) | 0.1730 | 0.021 | 4 |
ZnNiP2O7 (mvc-5701) | 0.1296 | 0.019 | 4 |
ZnCoP2O7 (mvc-5639) | 0.1705 | 0.024 | 4 |
MgCoP2O7 (mvc-5586) | 0.1166 | 0.035 | 4 |
NaLiCu(PO3)3 (mp-775900) | 0.5808 | 0.087 | 5 |
LiMn3P2(HO3)4 (mp-763726) | 0.6151 | 0.479 | 5 |
Na6Al4Fe(Si4O13)2 (mp-39647) | 0.6251 | 0.043 | 5 |
KNaZnP2O7 (mp-554157) | 0.5124 | 0.000 | 5 |
Na6Al4Fe(Si4O13)2 (mp-42298) | 0.6291 | 0.000 | 5 |
Li4Mn3CuNi2(PO4)6 (mp-775323) | 0.7225 | 0.080 | 6 |
Li4Mn3NbV2(PO4)6 (mp-770640) | 0.7209 | 0.095 | 6 |
NaLiMn2Fe4(PO4)6 (mp-777193) | 0.6981 | 0.018 | 6 |
Li4Mn3NbCr2(PO4)6 (mp-776566) | 0.6992 | 0.725 | 6 |
Li4TiMn3Cr2(PO4)6 (mp-778261) | 0.7149 | 0.081 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Mg_pv Ni_pv P O |
Final Energy/Atom-6.7158 eV |
Corrected Energy-323.8158 eV
-323.8158 eV = -295.4957 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 8.6560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)