Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.391 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.079 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBiO2 |
Band Gap0.186 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmc21 [26] |
HallP 2c 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 290.4 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 207.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 109.6 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 276.4 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 290.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 109.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 182.6 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 331.7 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 290.4 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 166.0 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 165.8 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 290.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 292.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 182.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 290.4 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 290.4 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 207.5 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 166.0 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 207.5 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 290.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 255.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 276.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 182.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 290.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 207.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 292.2 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 276.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 292.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 146.1 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 249.0 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 290.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 109.6 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 109.6 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 276.4 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 328.7 |
TePb (mp-19717) | <1 1 1> | <0 1 0> | 290.4 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 207.5 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 290.4 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 165.8 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 124.5 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 207.5 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 124.5 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 165.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 255.7 |
BN (mp-984) | <1 0 1> | <0 1 1> | 165.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 328.7 |
BN (mp-984) | <1 1 1> | <0 1 1> | 276.4 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 166.0 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 1> | 221.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 292.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NbV3O8 (mp-771572) | 0.3265 | 0.303 | 3 |
Mn12O5F19 (mp-763188) | 0.3617 | 0.070 | 3 |
Mn12O5F19 (mp-779834) | 0.3691 | 0.069 | 3 |
VCo3O8 (mp-765821) | 0.3766 | 0.114 | 3 |
Mn6OF11 (mp-774185) | 0.3728 | 0.040 | 3 |
Ti3Nb2V3O16 (mp-770898) | 0.3595 | 0.094 | 4 |
Mn3Nb2Fe3O16 (mp-775243) | 0.3575 | 0.099 | 4 |
V2Cr3Sb3O16 (mp-773383) | 0.3615 | 0.128 | 4 |
Mn2Co3Te3O16 (mp-769913) | 0.3605 | 0.125 | 4 |
Mn3V2Cr3O16 (mp-773144) | 0.3434 | 0.084 | 4 |
TiO2 (mvc-12404) | 0.4426 | 0.061 | 2 |
BiO2 (mvc-15392) | 0.4424 | 0.090 | 2 |
VO2 (mp-715553) | 0.4096 | 0.072 | 2 |
TiO2 (mvc-11500) | 0.4308 | 0.074 | 2 |
VO2 (mp-1021522) | 0.4303 | 0.033 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Bi O |
Final Energy/Atom-5.5178 eV |
Corrected Energy-143.6641 eV
-143.6641 eV = -132.4275 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)