Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.375 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.271 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.45 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToP2WO7 + Mg2P2O7 + W |
Band Gap1.994 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 305.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 -1 -1> | 223.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 210.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 -1 -1> | 223.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 308.0 |
InAs (mp-20305) | <1 1 0> | <1 -1 0> | 321.1 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 309.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 -1> | 263.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 -1 0> | 256.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 326.5 |
CdS (mp-672) | <0 0 1> | <1 -1 0> | 256.9 |
CdS (mp-672) | <1 0 0> | <1 -1 0> | 256.9 |
CdS (mp-672) | <1 0 1> | <0 1 -1> | 263.3 |
CdS (mp-672) | <1 1 1> | <1 -1 0> | 256.9 |
LiF (mp-1138) | <1 0 0> | <0 1 -1> | 263.3 |
LiF (mp-1138) | <1 1 0> | <1 -1 0> | 256.9 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 287.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 -1> | 158.0 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 220.0 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 305.4 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 261.7 |
YVO4 (mp-19133) | <1 0 0> | <1 -1 0> | 321.1 |
YVO4 (mp-19133) | <1 1 0> | <0 1 -1> | 316.0 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 143.6 |
AlN (mp-661) | <1 0 0> | <0 1 -1> | 158.0 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 143.6 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 218.1 |
AlN (mp-661) | <1 1 1> | <1 -1 0> | 256.9 |
TePb (mp-19717) | <1 0 0> | <1 -1 0> | 128.4 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 305.4 |
CeO2 (mp-20194) | <1 0 0> | <0 1 -1> | 316.0 |
CeO2 (mp-20194) | <1 1 0> | <1 1 -1> | 298.4 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 309.0 |
BaF2 (mp-1029) | <1 0 0> | <0 1 -1> | 158.0 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 220.0 |
Te2Mo (mp-602) | <1 0 1> | <1 -1 0> | 321.1 |
Ag (mp-124) | <1 0 0> | <1 -1 0> | 256.9 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 174.5 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 152.3 |
GaN (mp-804) | <1 0 0> | <1 -1 0> | 256.9 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 174.5 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 206.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 308.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 261.2 |
SiO2 (mp-6930) | <1 0 0> | <1 -1 0> | 192.7 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 239.3 |
SiO2 (mp-6930) | <1 1 1> | <1 -1 0> | 256.9 |
GaSe (mp-1943) | <0 0 1> | <1 -1 1> | 162.1 |
GaSe (mp-1943) | <1 0 1> | <1 0 -1> | 206.0 |
KCl (mp-23193) | <1 0 0> | <1 -1 0> | 128.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AgPO3 (mp-18702) | 0.5908 | 0.000 | 3 |
NaPO3 (mp-555118) | 0.5792 | 0.000 | 3 |
GePbO3 (mp-554699) | 0.5806 | 0.000 | 3 |
MgTe2O7 (mvc-6996) | 0.5915 | 0.279 | 3 |
Hg3(PO4)2 (mp-12199) | 0.5715 | 0.000 | 3 |
LiNi(PO3)3 (mp-861591) | 0.5099 | 0.091 | 4 |
Li4Cu(PO3)6 (mp-760683) | 0.5046 | 0.050 | 4 |
CuAs2PbO7 (mp-21560) | 0.5298 | 0.020 | 4 |
Li2SnP2O7 (mp-673071) | 0.4237 | 0.037 | 4 |
LiFe2(PO4)2 (mp-768323) | 0.5118 | 0.086 | 4 |
BaZn2As3HO11 (mp-758313) | 0.6774 | 0.011 | 5 |
LiFePH2O5 (mp-780200) | 0.7156 | 0.076 | 5 |
NaLi2B(PO4)2 (mp-1020646) | 0.6862 | 0.000 | 5 |
Na2LiCuP2O7 (mp-776424) | 0.7148 | 0.085 | 5 |
Li2SbSO4F3 (mp-769153) | 0.7086 | 0.069 | 5 |
KMg3AlSi3(O5F)2 (mp-684841) | 0.6754 | 0.215 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Mg_pv P W_pv O |
Final Energy/Atom-6.9891 eV |
Corrected Energy-172.2945 eV
-172.2945 eV = -153.7604 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction) - 8.7020 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)