Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.667 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.287 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.55 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToW8O21 + W |
Band Gap1.238 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 331.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 110.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 257.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 183.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 257.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 257.4 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 183.9 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 107.5 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 100.4 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 174.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 147.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 294.2 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 174.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 183.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 183.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 110.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 183.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 257.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 257.4 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 183.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 257.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 183.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 110.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 110.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 294.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 257.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 183.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 110.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 200.9 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 100.4 |
Te2W (mp-22693) | <1 0 1> | <0 1 0> | 100.4 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 200.9 |
TePb (mp-19717) | <1 0 0> | <0 1 1> | 215.0 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 294.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 257.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 331.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 36.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 147.1 |
BN (mp-984) | <1 0 0> | <0 1 1> | 215.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 257.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 110.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 331.0 |
Al (mp-134) | <1 0 0> | <0 0 1> | 257.4 |
Al (mp-134) | <1 1 0> | <0 0 1> | 183.9 |
Al (mp-134) | <1 1 1> | <0 0 1> | 110.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 100.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 257.4 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 183.9 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 147.1 |
CdTe (mp-406) | <1 0 0> | <0 1 1> | 215.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V3CoO8 (mp-861494) | 0.5398 | 0.177 | 3 |
Ti12Fe5O32 (mp-773987) | 0.5365 | 0.108 | 3 |
Ti6Co3O16 (mp-765900) | 0.5186 | 0.236 | 3 |
Li2Mn15O32 (mp-698551) | 0.5474 | 0.098 | 3 |
V3CoO8 (mp-868771) | 0.5398 | 0.177 | 3 |
MgCoAsO5 (mvc-5557) | 0.7321 | 0.182 | 4 |
Zn3Cu10(TeO6)6 (mvc-15145) | 0.6422 | 0.063 | 4 |
TaAl(WO4)2 (mvc-781) | 0.6623 | 0.297 | 4 |
CrO2 (mvc-5485) | 0.2950 | 0.388 | 2 |
TiO2 (mvc-5171) | 0.3432 | 0.171 | 2 |
WO2 (mvc-10363) | 0.2933 | 0.299 | 2 |
FeO2 (mvc-13234) | 0.2922 | 1.011 | 2 |
FeO2 (mvc-12204) | 0.3551 | 0.269 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: W_pv O |
Final Energy/Atom-7.3670 eV |
Corrected Energy-334.2778 eV
-334.2778 eV = -265.2109 eV (uncorrected energy) - 52.2120 eV (MP Advanced Correction) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)