Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.934 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.116 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.83 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoS2 + Co2S3 + CaS |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 292.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 167.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 208.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 292.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 292.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 167.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 292.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 292.4 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 208.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 167.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 334.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 334.2 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 115.0 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 250.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 292.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 208.9 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 199.2 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 115.0 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 208.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 292.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 125.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 167.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 167.1 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 292.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 292.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 208.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 167.1 |
Al (mp-134) | <1 1 0> | <0 0 1> | 334.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 167.1 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 208.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 292.4 |
Al (mp-134) | <1 0 0> | <0 0 1> | 334.2 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 292.4 |
C (mp-66) | <1 0 0> | <0 0 1> | 125.3 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 230.0 |
SiC (mp-7631) | <0 0 1> | <1 1 0> | 199.2 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 125.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 292.4 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 125.3 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 292.4 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 230.0 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 292.4 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 208.9 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 230.0 |
C (mp-66) | <1 1 0> | <1 1 0> | 199.2 |
C (mp-66) | <1 1 1> | <0 0 1> | 292.4 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 167.1 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 208.9 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 208.9 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 167.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca(FeS2)4 (mvc-13376) | 0.1341 | 0.326 | 3 |
Ca(NiS2)4 (mvc-11277) | 0.1307 | 0.172 | 3 |
Zn(CoS2)4 (mvc-11131) | 0.2414 | 0.127 | 3 |
Zn(SnO2)4 (mvc-8750) | 0.2191 | 0.214 | 3 |
Mg(SnO2)4 (mvc-8773) | 0.1930 | 0.206 | 3 |
LiMn3CrO8 (mp-780544) | 0.2574 | 0.056 | 4 |
LiCo3CuO8 (mp-761730) | 0.2707 | 0.060 | 4 |
LiCrCo3O8 (mp-763181) | 0.2681 | 0.141 | 4 |
LiMnCo3O8 (mp-778023) | 0.2705 | 0.013 | 4 |
LiTi3VO8 (mp-768011) | 0.2407 | 0.096 | 4 |
Co15O28 (mp-769432) | 0.5129 | 0.024 | 2 |
Ti8O13 (mp-752989) | 0.5719 | 0.010 | 2 |
Mn5O8 (mp-761290) | 0.3057 | 0.080 | 2 |
Co7O12 (mp-771737) | 0.5628 | 0.124 | 2 |
Ti8C5 (mp-27919) | 0.5560 | 0.000 | 2 |
Li4MnSn(WO6)2 (mp-775961) | 0.6979 | 0.050 | 5 |
Li4CrSb(TeO6)2 (mp-781050) | 0.7179 | 0.048 | 5 |
Li4FeBi(TeO6)2 (mp-776005) | 0.7165 | 0.036 | 5 |
Li4Cr2TeWO12 (mp-775566) | 0.7066 | 0.081 | 5 |
Li4Mn2TeWO12 (mp-768044) | 0.6995 | 0.054 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Co S |
Final Energy/Atom-5.4124 eV |
Corrected Energy-74.3848 eV
Uncorrected energy = -70.3608 eV
Composition-based energy adjustment (-0.503 eV/atom x 8.0 atoms) = -4.0240 eV
Corrected energy = -74.3848 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)