Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.045 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.060 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.37 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa2Nb2O7 + MnO |
Band Gap2.513 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 105.8 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 317.5 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 141.1 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 176.4 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 176.4 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 317.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 247.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 282.2 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 282.2 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 141.1 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 211.7 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 352.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 176.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 176.4 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 35.3 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 141.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 141.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 122.7 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 176.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 282.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 176.4 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 141.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 105.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 282.2 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 282.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 245.5 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 141.1 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 257.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 352.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 176.4 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 176.4 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 128.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 141.1 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 352.8 |
BN (mp-984) | <1 0 0> | <1 0 0> | 211.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 245.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 141.1 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 35.3 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 0> | 247.0 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 176.4 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 317.5 |
CdTe (mp-406) | <1 1 1> | <1 0 0> | 317.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 245.5 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 141.1 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 1> | 128.6 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 35.3 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 317.5 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 141.1 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 352.8 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 282.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tm2GeO5 (mp-756949) | 0.4606 | 0.100 | 3 |
Al2(BiO3)3 (mvc-12722) | 0.4730 | 0.124 | 3 |
Lu2GeO5 (mp-755373) | 0.4789 | 0.101 | 3 |
CdCoO3 (mp-770050) | 0.4450 | 0.051 | 3 |
Na2TeO4 (mp-560613) | 0.4443 | 0.000 | 3 |
Ca2Ta2NiO8 (mvc-2726) | 0.2269 | 0.269 | 4 |
Ca2Ta2CoO8 (mvc-2753) | 0.2284 | 0.096 | 4 |
Ca2Nb2NiO8 (mvc-530) | 0.1633 | 0.268 | 4 |
Ca2Nb2CoO8 (mvc-544) | 0.1164 | 0.162 | 4 |
Ca2Nb2FeO8 (mvc-644) | 0.0991 | 0.275 | 4 |
Pb3O4 (mp-636813) | 0.6334 | 0.038 | 2 |
Pb2O3 (mp-20078) | 0.5095 | 0.009 | 2 |
V7O13 (mp-556332) | 0.6292 | 0.038 | 2 |
V7O13 (mp-623373) | 0.6243 | 0.038 | 2 |
V5O9 (mp-704305) | 0.6313 | 0.008 | 2 |
Li4MnV(WO6)2 (mp-761440) | 0.5013 | 0.049 | 5 |
LaZnFeSbO6 (mvc-9031) | 0.5177 | 0.270 | 5 |
LaVZnCrO6 (mvc-9860) | 0.4949 | 0.247 | 5 |
NaLiV(OF)2 (mp-764851) | 0.5006 | 0.078 | 5 |
LaZnFeCoO6 (mvc-9020) | 0.5096 | 0.387 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Ca_sv Mn_pv Nb_pv O |
Final Energy/Atom-8.0957 eV |
Corrected Energy-225.0854 eV
-225.0854 eV = -210.4871 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 3.3617 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)